Please wait a minute...
金属学报  1996, Vol. 32 Issue (3): 278-283    
  论文 本期目录 | 过刊浏览 |
含FeO熔渣的起泡过程及起泡参数间关系分析
黄宗泽;肖兴国;肖泽强
东北大学
FOAMING BEHAVIOUR AND PARAMETERS OF FeO-BEARING SLAGS
HUANG Zongze;XIAO Hingguo;XIAO Zeqiang(Northeastern University; Shenyang 110006); S. D. SINGH(National Metallurgical Laboratory; Jamshedpur; India;831007) (Manuscript recieved 1995-06-29)
引用本文:

黄宗泽;肖兴国;肖泽强. 含FeO熔渣的起泡过程及起泡参数间关系分析[J]. 金属学报, 1996, 32(3): 278-283.
, , . FOAMING BEHAVIOUR AND PARAMETERS OF FeO-BEARING SLAGS[J]. Acta Metall Sin, 1996, 32(3): 278-283.

全文: PDF(349 KB)  
摘要: 对CaO-SiO2一Al2O3-FeO熔渣在石墨还原过程中的起泡行为的分析表明,熔渣的起泡率受渣中气体的产生速度及熔渣的起泡指数影响;熔渣的起泡指数随渣中气泡直径的增大而减小;随熔渣碱度的减小,泡沫渣的平均寿命延长,泡沫化愈稳定。而泡沫渣高度的变化是由渣中气体的产生速度和排出速度的差异决定的。
关键词 : 泡沫渣,  起泡指数,  起泡寿命,  含FeO渣    
Abstract:The foaming behaviour of CaO-SiO2-Al2O3-FeO slag system during its reduction process showed that the foaming ratio of the slag was influenced by the rate of the generated gas as well as the foaming index of the slag. The foaming index of the slag increased with decreasing the size of the bubbles inside the molten slag. With decreasing the basicity of the slag, the foaminess became more stable and the foaming life of the slag increased. The analysis of the foaming behaviour of the molten slag reveals that the height of the foaming slag is dependent on the difference between the rates of the gas generation within and discharge from the foam. Correspondent: XIAO Xingguo, professor, Department of Ferrous Metallurgy, Northeastern University,Shenyang 110006
Key words: foaming    foaming index    foaming life    FeO-bearing slag
收稿日期: 1996-03-18     
基金资助:国家自然科学基金
1黄宗泽,肖兴国,肖泽强,SinghSD.金属学报,1995;31:B2892黄宗泽,肖兴国,肖泽强,SinghSD,东北大学学报,1995;16:2883OgawaY,HuinD,GayeH,TokumitsuN.ISIJInt,1993;33:2244SzekelyJ.FluidFlowPhenomenainMetalsProcessing.AmericanAcademicPress,19795RoK,FruchanRJ.MetalTrans,1989;20B:5096FuwaT.TransJIM,1989;29:353
[1] 吴铿; 姚克虎 . 硼酸盐熔体中分解反应的发泡特性参数[J]. 金属学报, 2000, 36(12): 1248-1252 .
[2] 吴铿; 赵纪伟; 储少军; 王颖 . 硼酸盐熔体中内生气源发泡性能方程的发泡和消泡系数[J]. 金属学报, 1999, 35(7): 726-730 .
[3] 黄宗泽;肖兴国;肖泽强. CaO-SiO_2-Al_2O_3-FeO熔渣起泡行为的研究[J]. 金属学报, 1995, 31(19): 289-294.