| Ni-Fe-Cr-B-Si涂层超塑扩散焊接的强化效应及耐磨性 |
| 李延祥;文九巴;祝要民;黄金亮 |
| 洛阳工学院;西安交通大学 |
|
| STRENGTHENING AND WEAR RESISTANCE OF Ni-Fe-Cr-B-Si SPRAY ALLOY COATING BY SUPERPLASTICAL DIFFUSION WELDING |
| LI Yanxiang;WEN Jiuba;ZHU Yaomin(Luoyang Institute of Technology; Luoyang471039); HUANG Jinliang (Xi'an Jiaotong University; Xi'an 710049)(Manuscript received 1995-07-11) |
引用本文:
李延祥;文九巴;祝要民;黄金亮. Ni-Fe-Cr-B-Si涂层超塑扩散焊接的强化效应及耐磨性[J]. 金属学报, 1996, 32(5): 538-543.
,
,
,
.
STRENGTHENING AND WEAR RESISTANCE OF Ni-Fe-Cr-B-Si SPRAY ALLOY COATING BY SUPERPLASTICAL DIFFUSION WELDING[J]. Acta Metall Sin, 1996, 32(5): 538-543.
| 1AC著,刘春林译.金属与合金的超塑效应.北京:科学技术出版社,1983:542PillingJ,LiveseyDW,HawkyardJB,RidleyN.MetSci,1984;3:1173李延祥,文九巴,黄金亮,祝要民.金属学报,1994;30:B1364TangS著,宋玉泉,齐安民译.超塑性力学,长沙:湖南大学出版社,1989:365高彩桥.摩擦金属学.哈尔滨:哈尔滨工业大学出版社,1988:141-186 |
|