| Fe_3Al合金B2有序化过程的场离子显微镜观察 |
| 翁军;朱逢吾;职任涛;王双全;肖纪美 |
| 北京科技大学 |
|
| FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY |
| WENG Jun; ZHU Fengwu; ZHI Rentao; WANG Shuangquan; XIAO jimei (University of Scicnce and Technology Beijing; Beijing 100083)(Manuscript received 1995-12-18) |
引用本文:
翁军;朱逢吾;职任涛;王双全;肖纪美. Fe_3Al合金B2有序化过程的场离子显微镜观察[J]. 金属学报, 1996, 32(7): 695-699.
,
,
,
,
.
FIM OBSERVATION ON B2 ORDERING IN Fe_3Al ALLOY[J]. Acta Metall Sin, 1996, 32(7): 695-699.
| 1SouthworthHN,RalphB.PhilMag,1970;21:232TauntRJ,SinclairT,RalphB.PhysStatSolA,1973;16:4693KrauseHJ,WittigJE,FrommegerG.ZMetallkd,1987;78:5764WengJ,ZhuFW,XiaoJM.ZMetallkd,1994;85:4325MarcinkowskiMJ,BrownN.JApplPhys,1962;33:5376NewmanRW,HrenJJ.PhilMag,1967;16:2117LinY,ZhuF,XiaoJ.AclaMetallMater,1994;42:2499^ |
|