Please wait a minute...
金属学报  1997, Vol. 33 Issue (10): 1079-1084    
  论文 本期目录 | 过刊浏览 |
用Wilson方程估算多元液态合金在给定温度下的组元活度
陶东平;杨显万
昆明理工大学;昆明650093;昆明理工大学;昆明650093
ESTIMATION OF COMPONENT ACTIVITIES IN MULTICOMPONENT LIQUID ALLOYS AT GIVEN TEMPERATURES USING WILSON EQUATION
TAO Dongping;YANG Xianwan (Kunming University of Science and Technology;Kunming 650093)
引用本文:

陶东平;杨显万. 用Wilson方程估算多元液态合金在给定温度下的组元活度[J]. 金属学报, 1997, 33(10): 1079-1084.
, . ESTIMATION OF COMPONENT ACTIVITIES IN MULTICOMPONENT LIQUID ALLOYS AT GIVEN TEMPERATURES USING WILSON EQUATION[J]. Acta Metall Sin, 1997, 33(10): 1079-1084.

全文: PDF(418 KB)  
摘要: 根据Wilson参数与温度的关系,可将Wilson方程扩展到只利用不同温度下测定的二元液态合金各组元的活度,估算出给定温度下二元和多元液态合金各组元的活度.研究结果表明,多元液态合金的活度估算值与其实验数据符合良好.
关键词 : 活度估算,  多元液态合金,  Wilson方程    
Abstract:Based on the relationship between the Wilson parameters and temperature,the Wilson equation can be extended to estimating activities of components of binary and multicomponent liquid alloys at given temperatures only by using the activities of components of binary liquid alloys measured at some temperatures. The results show that the estimation values of activity of multicomponent liquid alloys are in good agreement with their experimental data of activity.
Key words: estimation of activity    multicomponent liquid alloys    Wilson equation
收稿日期: 1997-10-18     
1 Wilson G M.J amer Chem Soc,1964;86:127
2陶东平.金属学报,1991;27:B380
3Tao D P. Metall Trans B 1992; 23B(4):526
4陶东平.有色金属,1993;45(3):59
5Orye R V,Prausnitz J M, Indu Eng Chem,1965;57(5 ):18
6Hultgren R Desai P D, Hawkins D T Geiser M, Kelley K K. Selected Values of the Thermodynamic Properties of Binary alloys,Metals Park,Ohio:aSM,1973:1963
7Dealy J M,Pehlke R D Trans Metall Soc aIME 1963; 227:1030
8Lucas L D.In:Rapp R a eds,Physicochemical Measurements in Metals Research New York:JohnWiley& Sons, Inc, 1970: 219
9 MoserZ,Gasior W,Panek Z.Metall Trans B,1984;B15:543
10Moser Z Zakulski W, Jedrzejek C Z Metallkde, 1979;70:293
11 Ptak W,Moser Z.Trans Metall Soc aIME,1968;242:558
12 Prausnitz J M, Lichtenthaler R N, de azevedo E G. Molecuhr Thermodynamics of Fluid-PhaseEquilibria.2nd ed,Englewood Cliffis N J:Prentice—Hall Inc,1986:234
13 Walas S M著,韩世钩等译。化工相平衡北京:中国石化出版社,1991:221
[1] 陶东平. 用Wilson方程预测三元液态合金的热力学性质[J]. 金属学报, 1991, 27(6): 92-98.