Please wait a minute...
金属学报  1997, Vol. 33 Issue (4): 386-390    
  论文 本期目录 | 过刊浏览 |
疲劳断口分析的Fourier变换方法
颜云辉;王德俊;黄雨华;王清昊;王彤波
东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006
FOURIER TRANSFORM METHOD FOR ANALYSIS OF FATIGUE FRACTOGRAPHS
YAN Yunhui; WANG Dejun;HUANG Yuhua; WANG Qinghao; WANG Tongbo (Northeastern University; Shenyang 110006)(Manuscript received 1996-05-20; in revised form 1996-07-04)
引用本文:

颜云辉;王德俊;黄雨华;王清昊;王彤波. 疲劳断口分析的Fourier变换方法[J]. 金属学报, 1997, 33(4): 386-390.
, , , , . FOURIER TRANSFORM METHOD FOR ANALYSIS OF FATIGUE FRACTOGRAPHS[J]. Acta Metall Sin, 1997, 33(4): 386-390.

全文: PDF(1023 KB)  
摘要: 对疲劳断口图像进行恰当的图像变换处理,可以从其丰富而复杂的图像信息中提取重要的有用特征,实现疲劳断口的定量分析。本文应用二维离散Fourier变换对疲劳断口表面图像进行分析处理后,再通过二次特征提取将二维图像分析转化为对两个一维特征波形的分析,从而有利于获得更为明确的有关疲劳断口的纹理特征和疲劳条纹的方向特征。研究结果表明,利用二维离散Fourier变换在空频域上对疲劳断口图像进行分析,可以获得在单纯空间域上所无法得到的疲劳断口图像的特征表征,这为进一步开展疲劳断口的定量分析研究提供了一条有效的新途径。
关键词 断口分析特征提取图像处理    
Abstract:The quantitative analysis for fatigue fractography can be realized through the suitable image transform of fatigue fractographs, from which some useful characteristics can be obtained. Two-dimensional discrete Fourier transform is used in the process of fatigue fractograph, and the important characteristics to describe the texture and direction features on a fatigue fracture surface are abstracted from the Fourier power spectrum. A two-dimensional image analysis problem can be simplified as a one-dimensional characteristic curve analysis. The results show that some important characteristics on a fatigue fracture surface can be obtained in space frequency domain by means of two-dimensional discrete Fourier transform, which are impossibly acquired in space domain of fractograph. The method presented in this paper is identified to be a new way to carry out quantitative analysis of fatigue fractography.
Key wordsanalysis of fracture surface    abstract of characteristic    image processing
收稿日期: 1997-04-18     
基金资助:国家教委留学回国人员科研基金;;冶金工业部自然科学基金;;国家教委博士点基金
1Strauss B M,Cullen W H.Fractography in Failure Analysis Philadelphia,Pa:ASTM Special Technical Publication 645,1978:73
2Gilbertson L N,Zipp R D.Fractography and Materials Science.Philadelphia,Pa:ASTM SpecialTechnical Publication 733,1981:355
3胡世炎.破断故障金相分析.北京:国防工业出版社,1979:202
4Koterazawa R,Ebara R,Nishida S,Fractography,London:Elsevier Applied Science,1990:220
5颜云辉,见新一。机械工程学报,1995;31(5):29
6颜云辉,王德俊。金属学报,1996;32(5):552
7Wahl F M著。王宗海,张存桢,吕英,肖芾译。数字图像信号处理,上海:远东出版社,1993:31
8陈廷标,夏良正.数字图像处理北京:人民邮电出版社,1990:73#
[1] 董旭光,付俊伟,杨院生. Al和Zn对铸造Mg-5Sn合金微观组织和力学性能的影响[J]. 金属学报, 2013, 49(5): 621-628.
[2] 姜文辉;姚向东;管恒荣;胡壮麒. DZ40M合金高温低周疲劳性能及其断口分析[J]. 金属学报, 1998, 34(4): 378-383.
[3] 于瀛大;平德海;彭红樱;李斗星;叶恒强. 能量过滤成像技术在材料研究中的应用[J]. 金属学报, 1997, 33(3): 233-240.
[4] 颜云辉;王德俊. 图像处理技术与金属断口分析[J]. 金属学报, 1996, 32(5): 552-556.
[5] 杨蕴林;李志;李炎. 恒温超塑焊接接头断口分析[J]. 金属学报, 1995, 31(20): 384-38.