| 疲劳断口分析的Fourier变换方法 |
| 颜云辉;王德俊;黄雨华;王清昊;王彤波 |
| 东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006;东北大学;沈阳;110006 |
|
| FOURIER TRANSFORM METHOD FOR ANALYSIS OF FATIGUE FRACTOGRAPHS |
| YAN Yunhui; WANG Dejun;HUANG Yuhua; WANG Qinghao; WANG Tongbo (Northeastern University; Shenyang 110006)(Manuscript received 1996-05-20; in revised form 1996-07-04) |
引用本文:
颜云辉;王德俊;黄雨华;王清昊;王彤波. 疲劳断口分析的Fourier变换方法[J]. 金属学报, 1997, 33(4): 386-390.
,
,
,
,
.
FOURIER TRANSFORM METHOD FOR ANALYSIS OF FATIGUE FRACTOGRAPHS[J]. Acta Metall Sin, 1997, 33(4): 386-390.
1Strauss B M,Cullen W H.Fractography in Failure Analysis Philadelphia,Pa:ASTM Special Technical Publication 645,1978:73 2Gilbertson L N,Zipp R D.Fractography and Materials Science.Philadelphia,Pa:ASTM SpecialTechnical Publication 733,1981:355 3胡世炎.破断故障金相分析.北京:国防工业出版社,1979:202 4Koterazawa R,Ebara R,Nishida S,Fractography,London:Elsevier Applied Science,1990:220 5颜云辉,见新一。机械工程学报,1995;31(5):29 6颜云辉,王德俊。金属学报,1996;32(5):552 7Wahl F M著。王宗海,张存桢,吕英,肖芾译。数字图像信号处理,上海:远东出版社,1993:31 8陈廷标,夏良正.数字图像处理北京:人民邮电出版社,1990:73# |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|