| Zr50Cu50合金过冷熔体中的晶体生长速度 |
| 王强;马明臻;张新宇;刘日平 |
| 燕山大学亚稳材料制备技术与科学国家重点实验室 |
|
| CRYSTAL GROWTH VELOCITY IN UNDERCOOLED Zr50Cu50 ALLOY MELT |
| WANG Qiang;MA Mingzhen;ZHANG Xinyu;LIU Riping |
| State Key Laboratory of Metastable Materials Science & Technology; Yanshan University |
引用本文:
王强 马明臻 张新宇 刘日平 . Zr50Cu50合金过冷熔体中的晶体生长速度[J]. 金属学报, 2008, 44(12): 1415-1418.
,
,
,
.
CRYSTAL GROWTH VELOCITY IN UNDERCOOLED Zr50Cu50 ALLOY MELT[J]. Acta Metall Sin, 2008, 44(12): 1415-1418.
[1]Schleip E,Willnecker R,Herlach D M,G(?)erler G P.Mater Sci Eng,1988;98:39 [2]Herlach D M.Annu Rev Mater Sci,1991;21:23 [3]Panofen C,Herlach D M.Mater Sci Eng,2007;A449-451: 699 [4]Galenko P K,Reutzel S,Herlach D M,Danilov D,Nestler B.Acta Mater,2007;55:6834 [5]Willnecker R,Herlach D M,Feuerbache B.Phys Rev Lett, 1989;62:12707 [6]Aoyama T,Paradis P,Ishikawa T,Yoda S.Mater Sci Eng, 2004;A375-377:460 [7]Li D L,Volkmann T.Eckler K,Herlach D M.J Crystal Growth,1995;152:101 [8]Li D,Herlach D M.Phys Rev Lett,1996;77:1801 [9]Eckler K,Norman F A,G(?)rtner F,Greet A L,Herlach D M.J Crystal Growth,1997;1-3:528 [10]Eckler K,Cochrane R F,Herlach D M,Feuerbacher B. Mater Sci Eng,1991;A133:702 [11]Barth M,Eckler K,Herlach D M.Mater Sci Eng,1991; A133:790 [12]Zhang J Y,Wang H R,Shi Z Q,Teng X Y,Ye Y F,Min G H.J Mater Sci Eng,2002;20:461 (张均艳,王焕荣,石志强.腾新营,叶以富,闵光辉.材料科学与工程,2002;20:461) [13]Wu N Q,Su L Z,Yuan M Y.Mater Sci Eng,1998;A257: 357 [14]Saida J,Matsushita M.J Mater Sci,2000;35:3539 [15]Ahounian Z,Tu G H,Strom-Olsen J O.J Appl Phys, 1982;53:4755 [16]Wang N,Li C,Du Z,Wang F,Zhang W.Comput Coupl Phase Diag Thermochem,2006;30:461 [17]Wang W H,Lewandowski J J,Greet A L.J Mater Res, 2005;20:2307 [18]Wang D,Li Y,Sun B B,Sui M L,Lu K,Ma E.Appl Phys Lett,2004;84:4029 [19]Fan G J,Fecht H,Lavemia E J.Appl Phys Lett,2004;84: 487 [20]Kawamura Y,Inoue A.Appl Phys Lett,2000;77:1114 [21]Turnbull D.ConCern Phys,1969;10:473 [22]Fan G L,Freels M,Choo H,Liaw P K,Li J J Z,Rhim W K,Johnson W L,Yu P,Wang W H.Appl Phys Lett,2006; 89:241917 [23]Ngai K L.J Phys Chem,1999;103B:10684 [24]Rah K,Eu B C.Phys Rev,2003;68E:051204 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|