| 高拉速板坯连铸结晶器液体摩擦机理分析 |
| 孟祥宁;朱苗勇 |
| 东北大学材料与冶金学院 |
|
| ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED |
| Xiang-Ning MENG;Miao-Yong ZHU |
| 东北大学 |
引用本文:
孟祥宁; 朱苗勇 . 高拉速板坯连铸结晶器液体摩擦机理分析[J]. 金属学报, 2008, 44(10): 1193-1197 .
,
.
ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED[J]. Acta Metall Sin, 2008, 44(10): 1193-1197 .
[1]Yao M,Wang W H,Wei S L,Yin H B,Fang D C.J Dalian Univ Technol,2002;42:195 (姚曼,王文华,魏树立,尹合壁,方大成.大连理工大学学报,2002:42:195) [2]Li X K,Zhang D M.Continuous Casting Mold Oscillation Technology.Beijing:Metallurgical Industry Press,2000: 30 (李宪奎,张德明.连铸结晶器振动技术.北京:冶金工业出版社,2000:30) [3]Hwang Y S,Cha P R,Nam H S,Moon K H,Yoon J K. ISIJ Int,1997;37:659 [4]Zhang J M,Zhang L,Wang X H,Wang L F.Acta Metall Sin,2003;39:1285 (张炯明,张立,王新华,王立峰.金属学报,2003;39:1285) [5]Okazawa K,Kajitani T,Yamada W,Yamamura H.ISIJ Int,2006;46:226 [6]Meng X N,Zhu M Y,Liu X D,Cheng N L,Jiang Z K. Acta Metall Sin,2007;43:205 (孟祥宁,朱苗勇,刘旭东,程乃良,江中块.金属学报,2007;43:205) [7]Takeuchi E,Brimacombe J K.Metall Trans,1984;15B: 493 [8]Suzuki M,Mizukami H,Kitagawa T,Kawakami K,Uchida S,Komatsu Y.ISIJ Int,1991;31:254 [9]Mizukami H,Kawakami K,Kitagawa T,Suzuki M,Uchida S,Komatsu Y.Tetsu Hagané,1986;72:1862 (水上秀昭,川上公成,北川融,铃木干雄,内田繁孝,小松喜美.铁と钢,1986;72:1862) [10]Zhang H B,Wang H Z.Iron Steel,1995;30(11):17 (张洪波,王海之.钢铁,1995;30(11):17) [11]Kajitani T,Okazawa K,Yamada W,Yamamura H.ISIJ Int,2006;46:1432 [12]Meng Y,Thomas B G.ISIJ Int,2006;46:660 [13]Meng X N,Zhu M Y.Chin Mech Eng,2007;18:1779 (孟祥宁,朱苗勇.中国机械工程,2007;18:1779) [14]Sumi I,Shimizu H,Nishioka S,Nakada M,Murakami K, Suzuki M.ISIJ Int,2003;43:807 [15]Meng X N,Zhu M Y,Cheng N L.Acta Metall Sin,2007; 43:839 (孟祥宁,朱苗勇,程乃良金属学报,2007;43:839) [16]Yukio N,Youichi F.ISIJ Int,1984;24:1262 [17]Gan Y,Chen D L,Yang W G.Iron Steel,1999;34(4):16 (干勇,陈栋梁,杨文改.钢铁,1999;34(4):16) [18]Zang X Y,Wang X D,Ma Y,Yao M,Zhang L.Iron Steel, 2007;42(10):39 (臧欣阳,王旭东,马勇,姚曼,张立.钢铁,2007;42(10):39) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|