| 基于MacPherson-Srolovitz 拓扑依赖速率方程的三维晶粒尺寸分布研究 |
| 王浩;刘国权 |
| 北京科技大学材料科学与工程学院新金属材料国家重点实验室 |
|
| STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION |
| ; |
引用本文:
王浩; 刘国权 . 基于MacPherson-Srolovitz 拓扑依赖速率方程的三维晶粒尺寸分布研究[J]. 金属学报, 2008, 44(7): 769-774 .
,
.
STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION[J]. Acta Metall Sin, 2008, 44(7): 769-774 .
[1]Hillert M.Acta Metall,1965;13:227 [2]Atkinson H V.Acta Metall,1988;36:469 [3]Mullins W W.J Appl Phys,1956;27:900 [4]Yu H B.Doctorate Dissertation,University of Science and Technology Beijing,1997 (于海波.北京科技大学博士学位论文,1997) [5]Yu H B,Liu G Q.China Sci Bull,1996;41:2000 (于海波,刘国权.科学通报,1996;41:2000) [6]Liu G Q,Song X Y,Yu H B,Gu N J.Acta Metall Sin, 1999;35:245 (刘国权,宋晓艳,于海波,谷南驹.金属学报,1999;35:245) [7]Wang C,Liu G Q,Yu H B.Acta Metall Sin,2004;40: 1233 (王超,刘国权,于海波.金属学报,2004;40:1233) [8]MacPherson R D,Srolovitz D J.Nature,2007;446:1053 [9]Hilgenfeldt S,Kraynik A M,Koehler S A,Stone H A.Phys Rev Left,2001;86:2685 [10]Hilgenfeldt S,Kraynik A M,Reinelt D A,Sulliwan J M. Europhys Left,2004;67:484 [11]Glicksman M E.Philos Mag,2005;85:3 [12]Rios P R,Glicksman M E.Acta Mater,2006;54:1041 [13]Kinderlehrer D.Nature,2007;446:995 [14]Wang H,Liu G Q.Acta Metall Sin,2008;44:13 (王浩,刘国权.金属学报,2008;44:13) [15]Brown L C.Acta Metall,1989;37:71 [16]Coughlan S D,Fortes M A.Scr Metall Mater,1993;28: 1471 [17]Zhang C,Suzuki A,Ishimaru T,Enomoto M.Metall Mater Trans,2004;35A:1927 [18]Weygand D,Brechet Y,Lepinoux J,Gust W.Philos Mag, 1999;79B:703 [19]Wakai F,Enomoto N,Ogawa H.Acta Mater,2000;48: 1297 [20]Krill C E,Chen L Q.Acta Mater,2002;50:3057 [21]Wang H,Liu G Q,Qin X G.J Univ Sci Technol Beijing, in press (王浩,刘国权,秦湘阁.北京科技大学学报,待发表) [22]Wang C,Liu G Q.Sci China,2004;47E:112 [23]Rios P R.Scr Mater,1999;40:665 [24]Rios P R.Scr Mater,1999;41:1283 [25]Rios P R.Scr Mater,2006;54:1633 [26]Wang C,Liu G Q,Wang G F,Xue W B.Mater Sci Eng, 2007;A454—455:547 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|