| 高硼铁基合金在不同铸型中凝固组织与力学性能的影响 |
| 刘仲礼;李言祥;陈祥;胡开华 |
|
| Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy |
| ;;; |
引用本文:
刘仲礼; 李言祥; 陈祥; 胡开华 . 高硼铁基合金在不同铸型中凝固组织与力学性能的影响[J]. 金属学报, 2007, 43(5): 477-481 .
,
,
,
.
Effect of Solidification Condition on Structure and Properties of High Boron Iron-Base Alloy[J]. Acta Metall Sin, 2007, 43(5): 477-481 .
[1] Guo C Q, Gao S Z. Foundry, 2004; 53: 761 (郭长庆,高守忠.铸造,2004;53:761) [2] Gol'dshtein Y E, Mizin V G. Met Sci Heat Treat, 1989; 30: 479 [3] Egorov E D, Sapozhnikov Yu L, Shakhnazarov Yu V. Met Sci Heat Treat, 1989; 31: 387 [4] Lorinczi J, Kralik G, Kovaces M, Horvath A. Mater Sci Forum, 2003; 414-415: 267 [5] Baarman M H. Scand J Metall, 1998; 27: 157 [6] Okita T, Wolfer W G, Garner F A, Sekimura N. J Nucl Mater, 2004; 329-333: 1013 [7] Middleham T H, Rait J R, Colbeck E W. J Iron Steel Inst, 1957; 187(1): 1 [8] Llewellyn D T. Ironmaking Steelmaking, 1993; 20: 338 [9] Taylor K A, Hansen S S. Metall Trans, 1990; 21A: 1706 [10] Wang X M, He X L. ISIJ Int, 2002; 42(Suppl.): 38 [11] The First Steel Works of Benxi Steel Corp. Boron Steel. Beijing: Metallurgical Industry Press, 1977: 2 (本溪钢铁公司第一炼钢厂.硼钢.北京:冶金工业出版社,1977: 2) [12] Ren Y H. Spec Steel, 1992; 13(5): 57 (任元和.特殊钢,1992;13(5):57) [13] Abenojar J, Velasco F, Martinez M A. J Mater Process Technol, 2003; 143-144: 28 [14] Palumbo M, Cacciamani G, Bosco E, Baricco M. Inter- metallics, 2003; 11: 1294 [15] Yang C L, Yang G C, Liu F, Chen Y Z, Liu N, Chen D, Zhou Y H. Physica, 2006; 373B: 136L |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|