| 固体透氧膜法制备金属Ta |
| 程红伟; 鲁雄刚; 李谦; 刘建民; 丁伟中; 周国治 |
| 上海大学材料科学与工程学院 |
|
| A NOVEL TECHNOLOGY TO PRODUCE METAL TANTALUM DIRECTLY FROM Ta2O5 |
| ;;;;; |
| School of Materials Science and Engineering; Shanghai University; |
引用本文:
程红伟; 鲁雄刚; 李谦; 刘建民; 丁伟中; 周国治 . 固体透氧膜法制备金属Ta[J]. 金属学报, 2006, 42(5): 500-504 .
,
,
,
,
,
.
A NOVEL TECHNOLOGY TO PRODUCE METAL TANTALUM DIRECTLY FROM Ta2O5[J]. Acta Metall Sin, 2006, 42(5): 500-504 .
[1] He J L. Chin J Rare Met, 2003; 27: 23 (何季麟.稀有金属,2003;27:23) [2] He J L. Eng Sci, 2003; 5(5): 40 (何季麟.中国工程科学,2003;5(5):40) [3] He J L, Zhang Z G, Xu Z T. Rare Met Mater Eng, 1998; 27: 9 (何季林,张宗国,徐忠亭.稀有金属材料与工程,1998;27: 9) [4] He J L. Eng Sci, 2001; 3(12): 85 (何季麟.中国工程科学,2001;3(12):85) [5] Lu X G, Zhou G Z, Ding W Z, Jang G C, Xu K D. J Iron Steel Res, 2003; 15(5): 69 (鲁雄刚,周国治,丁伟中,蒋国昌,徐匡迪.钢铁研究学报, 2003;15(5):69) [6] Pal U. JOM, 2001; 53(10): 25 [7] Pal U, Woolley D E,Kenney G B. JOM, 2001; 53(10): 32 [8] Woolley D E, Pal U. JOM, 2001; 53(10): 40 [9] Krishnan A, Lu X G, Pal U. Mater Metall Trans, 2005; 36B: 463 [10] Chen G Z, Fray D J, Farthing T W. Nature, 2000; 407: 361 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|