| FeMoSiB纳米晶合金薄带的脆性断裂 |
| 甘阳 周本濂 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
甘阳; 周本濂 . FeMoSiB纳米晶合金薄带的脆性断裂[J]. 金属学报, 2000, 36(4): 356-358 .
[1] Lu K, Wang J T, Wei W D. J Appl Phys, 1991; 69: 522 [2] Lu K. Mater Sci Eng, 1996; 16R: 161 [3] Sui M L, Pain S, He Y Z. Scr Metall Mater, 1991; 25:1537 [4] Lu K, Wei W D, Wang J T. Scr Metall Mater, 1990; 24:2319 [5] Tiberto P, Stantero A, Baricco M, Makto I, Duhaj P.Nanostruct Mated 1996; 7: 619 [6] Leonhard A, Xing L Q, Heilmaier M, Gebert A, Eckert J,Schultz L. Nanoatruct Mater 1998; 9: 805 [7] Liu X D, Wang J T, Ding B Z. Scr Metall Mater, 1993;28: 59 [8] Olofinjana A O, Davies H A. Nanostruct Mater 1995; 6:465 [9] Olofinjana A O, Kern J H, Davies H A. Mater Lett, 1994;20: 6 [10] Field J E. Contemp Phgs, 1971; 12: 1 [11] Johnson J W, Holloway D G. Philos Mag, 1966; 14: 731 |
|