| 真空感应熔炼超纯净镍基高温合金脱氮的研究 |
| 牛建平 杨克努 金涛 孙晓峰 管恒荣 胡壮麒 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
牛建平; 杨克努; 金涛; 孙晓峰; 管恒荣; 胡壮麒 . 真空感应熔炼超纯净镍基高温合金脱氮的研究[J]. 金属学报, 2001, 37(9): 943-946 .
[1] Michell A. In: Fu J, Zhang R S, Xie X S eds. Proceedingsof the 1Oth International Conference on Vacuum Metal-lurgy, Vol.1, Beijing: Metallurgical Industry Press, 1990:1 [2] Ford D A, Hooper P R, Jennings P A. In: Betz W,Liebowitz H, Perrone N eds, Proc Conf on High Tem-perature Alloy for Gas Turbines and Other Applications,Liege: Pergamon Press, 1986: 51 [3] Simkovich A. J Met, 1966; 4: 504 [4] Pehlke R D, Rizescu C. J Iron Steel Inst, 1971; 10: 776 [5] Rupp S, Bienvenu Y, Massol J, Ablitzer D. In: Betz WLiebowitz H, Perrone N. Proc Conf on High TemperatureAlloy for Gas Turbines and Other Applications, Liege:Pergamon Press, 1986: 787 [6] Liu Y H. Refractory, 1998; 32. 149(刘彦海 耐火材料,1998;32:149) [7] Humbert J C, Elliott J F.Trans Metall Soc AIME, 1960;218: 1076 [8] Wada H, Pehlke R D. Metall Trans, 1977; 8B: 443 [9] Sigworth G K, Elliot J F. Met Sci, 1974; 8: 298 [10] Pehlke R D, Elliott J F. Trans Metall Soc AIME, 1963;227: 844 [11] Ya S B, Ishii F, Iguchi Y, Nagasaka T. Metall Trans, 1977;19B: 233 [12] Helmut K, Oeters F. Arch Eisenhutten Wesen, 1962; 11:729 [13] Ya S B, Shinohara J, Tozaki H, Fuwa T. Tetsu Hagane,1974: 10: 1443(万谷志郎,倏原忠广,户崎秀男,不破祜.铁 钢,1974;10:1443) [14] Rao Y K, Lee H G. Iron Steelmak, 1985; 12: 209 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|