| 高Ti炉渣中Ca-Ti矿相析出过程的计算机模拟 |
| 李晨曦 隋智通 李玉海 |
| 沈阳工业大学材料科学与工程学院;沈阳 110023 |
|
引用本文:
李晨曦; 隋智通; 李玉海 . 高Ti炉渣中Ca-Ti矿相析出过程的计算机模拟[J]. 金属学报, 2001, 37(7): 763-766 .
[1] Wang X Q. V-Ti-Bearing Magnetite Ore Smelting ina Blast Furnace. Beijing: Metallurgical Industry Press,1994: 106 (王喜庆.钒钛磁铁矿高炉冶炼.北京:冶金工业出版社,1994:106) [2] Du H G. Principle of V-Ti-Bearing Magnetite Ore Smelting in a Blast Furnace. Beijing: Science Press, 1996: 178 (杜鹤桂.高炉冶炼钒钛磁铁矿原理.北京:科学出版社,1996:178) [3] Lou T P, Li Y H, Ma J W, Xia Y H, Sui Z T. Acta MetallSin, 1999; 35: 834 (娄太平,李玉海,马俊伟,夏玉虎,隋智通.金属学报,1999;35:834) [4] Lou T P, Li Y H, Li L S, Sui Z T. Acta Metall Sin, 2000;36: 141 (娄太平,李玉海,李辽沙,隋智通.金属学报,2000;36:141) [5] Nastac L, Stefanescu M M. Metall Mater Trans, 1996;27A: 4075 [6] Nastac L, Stefanescu M M. Metall Mater Trans, 1996;27A: 4061 [7] Nastac L, Stefanescu M M. AFS Trans, 1996: 425 [8] Stefanescu M M, Pang H. Can Metall Q, 1998; 3-4: 229 |
|