| Au/NiCr/Ta和Au/NiCr多层金属膜的划痕特征载荷 |
| 唐武 马幼平 徐可为 王平 李弦 |
| 西安交通大学金属材料强度国家重点实验室;西安710049 |
|
引用本文:
唐武; 马幼平; 徐可为; 王平; 李弦 . Au/NiCr/Ta和Au/NiCr多层金属膜的划痕特征载荷[J]. 金属学报, 2002, 38(4): 407-410 .
[1] Kraatz P, Lee T H, Weil L, Thin Solid Films, 1997; 308-309: 375 [2] Jain A. Surf Coat Technol, 1998; 103-104(5): 20 [3] Fujinami Y, Hayashi H, Ebe A, Imai O, Ogata K. MaterChem Phys, 1998; 54: 102 [4] Gupta V, Hernandez R, Wu J X, Charconnet P. Vacuum,2000; 59: 292 [5] Baumann J, We rner T, Ehrlich A, Rennau M, KaufmannCh, Gessner T. Microelectron Eng, 1997; 37-38: 221 [6] Pauskardt R H, Lane M, Ma Q, Krishna N. Eng FractMech, 1998; 61: 141 [7] Lchimura H, Rodrigo A. Surf Coat Technol, 2000; 126(4):152 [8] Xie Z W, Zhu J. Thin Solid Films, 1998; 315(3): 192 [9] Randall N X, Favaro G, Frankel C H, Surf Coat Technol,2001; 137(3): 146 [10] Efeoglu I, Arnell R D. Thin Solid Films, 2000; 377-378(10): 346 [11] Xie F, Yuan J W, Xu K W, He J W. Surf Coat Technol,1999; 112(2): 236 |
|