| 复合体材料CuFe2O4-Pb(Mg1/3Nb2/3)O3的内耗和介电损耗 |
| 李伟 宋春花 包鹏 马骏 朱劲松 王业宁 |
| 南京大学物理系固体微结构国家重点实验室;南京210093 |
|
引用本文:
李伟; 宋春花; 包鹏; 马骏; 朱劲松; 王业宁 . 复合体材料CuFe2O4-Pb(Mg1/3Nb2/3)O3的内耗和介电损耗[J]. 金属学报, 2003, 39(11): 1197-1200 .
[1] Maheshkumar M, Srinivas A, Suryanarayana SV, KumarG S. Bull Mater Sci, 1998; 21: 251 [2] Lopatin S, Lapatona I, Lisnevskaya I. Ferroelectrics, 1994;162: 63 [3] Suryanaryana SV. Bull Mater Sci, 1994; 17: 1259 [4] Nan C-W. Phys Rev, 1994; 50B: 6082 [5] Boomgaard J V, Born R A J. J Mater Sci, 1978; 13: 1538 [6] Patankar K K, Patil S A, Sivakumar K V, Mahajan R P,Kolekar Y D, Kothale M B. Mater Chem Phys, 2000; 65:97 [7] Upadhyay S, Kumar D, Parkash O. Bull Mater Sci, 1996;19: 513 [8] Goodenough J B, Loeb A L. Phys Rev, 1955; 98: 391 [9] Tang X X, Manthiram A, Goodenough J B. J Solid StateChem, 1989; 79: 250 |
|