| 金属间化物Nd(Fe1-xCox)10V2的磁性能机制 |
| 罗广圣 曾贻伟 |
| 南昌大学化学与材料科学学院;南昌 330047 |
|
引用本文:
罗广圣; 曾贻伟 . 金属间化物Nd(Fe1-xCox)10V2的磁性能机制[J]. 金属学报, 2002, 38(3): 326-330 .
[1]Han X F, Yang F M, Zhu J J, Pan H G, Wang Y G, WangJ L, Tang N, Zhao R W. J Appl Phys, 1997; 81: 3248 [2]Wang J L, Tang N, Bruck E, Zhao R W, Yang F M, deBoer F R. J Appl Phys, 1997; 81: 5131 [3]Shen B G, Cheng Z H, Liang B, Guo H Q, Zhang J X,Gong H Y, Wang F W, Yan Q W, Zhan W S. Appl PhysLett, 1995; 67: 1621 [4]Yang Y C, Sun H, Zhang Z Y, Shen B G, Hu B P, de BoerF R. Sol Stat Commun, 1988; 68: 175 [5]Shiga M, Nakamura Y. J Phys Soc Jpn, 1976; 40: 1295 [6]Wang J L, Tang N, Yang D, Yang F M, de Boer F R. ActaPhys Sin, 1999; 48(suppl): 74 [7]Wang Y Z, Hu B P, Song L, Sheng B G. J Phys CondenMatter, 1999; 6: 7085# |
|