| TiNi薄膜马氏体稳定化及其形状记忆效应研究 |
| 刘晓鹏 金伟 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
刘晓鹏; 金伟 . TiNi薄膜马氏体稳定化及其形状记忆效应研究[J]. 金属学报, 2002, 38(2): 193-195 .
[1] Ishida A, Sato M, Miyazaki S. Mater Sci Eng A, 1999;273-275: 754 [2] Matsunaga T, Kajiwara S, Ogawa K, Kikuchi T, MiyazakiS. Mater Sci Eng A, 1999; 273-275: 745 [3] Sato M, Ishida A, Miyazaki S. Thin Solid Film, 1998; 315:305 [4] Kohl M, Dittmann D, Quandt E, Winzek B, Miyazaki S,Allen D M. Mater Sci Eng A, 1999; 273-275: 784 [5] Bendahan M, Aguir K, Seguin J L, Carchano H. Sens Ac-tuat, 1999; 74: 242 [6] Liu Y, Xie Z, Van Humbeeck J, Delaey L. Scr Mater, 1999;41: 1273 [7] Liu Y, Xie Z, Van Humbeeck J, Delaey L. Acta Mater,1998; 46: 4325 [8] Piao M, Otsuka K, Miyazaki S, Horikawa H. Mater TransJIM ,1993; 34: 919 [9] Liu Y N, Liu Y, Van Humbeeck J. Acta Mater, 1999; 47:199 [10] Liu Y, Favier D. Acta Mater, 2000; 48: 3489 [11] Pelosin V, Riviere A. Metall Mater Trans A, 1998, 29A:1175 [12] Miyazaki S, Igo Y, Otsuka K. Acta Mater, 1986; 34: 2045 |
|