激光快速熔凝Zn--2%Cu包晶合金的显微组织 |
苏云鹏 王 猛 林 鑫 李华琳 黄卫东 |
西北工业大学凝固技术国家重点实验室; 西安 710072 |
|
Microstructure of Zn-2%Cu Alloy Under Laser Rapid Melting—Solidification |
SU Yunpeng; WANG Meng; LIN Xin; LI Hualin; HUANG Weidong |
State Key Laboratory of Solidification Processing; Northwestern Polytechnical University; Xi'an 710072 |
引用本文:
苏云鹏; 王猛; 林鑫; 李华琳; 黄卫东 . 激光快速熔凝Zn--2%Cu包晶合金的显微组织[J]. 金属学报, 2005, 41(1): 67-.
,
,
,
,
.
Microstructure of Zn-2%Cu Alloy Under Laser Rapid Melting—Solidification[J]. Acta Metall Sin, 2005, 41(1): 67-.
[1] Wang M, Lin X, Su Y P, Shen S J, Huang W D. Mater Sci Eng, 2002; 1: 111(王猛,林鑫,苏云鵬,沈淑娟,黄卫东.材料科学与工程,2002;1:111) [2] Lee J H, Verhoeven J D. J Cryst Growth, 1994; 144: 353 [3] Busse P, Meissen F. Scr Mater, 1997; 36: 653 [4] Vandyoussefi M, Kerr H W, Kurz W. Acta Mater, 2000;48: 2297 [5] Xu W, Ma D, Feng Y P, Li Y. Scr Mater, 2001; 44: 631 [6] Liu Y C, Yang G C, Zhou Y H. J Cryst Growth, 2002;240: 603 [7] Singh J. J Mater Sci, 1994; 29: 5232 [8] Zimmerman M, Carrad M, Gremaud M, Kurz W. MaterSci Eng A, 1991; 134: 1278 [9] Gill S C, Zimmerman M, Kurz W. Acta Metall Mater,1992; 40: 2895 [10] Yang S, Huang W D, Liu W J, Su Y P, Zhou Y H. ChinJ Lasers, 2002; 29: 475(杨森,黄卫东,刘文今,苏云鹏,周尧和.中国激光,2002;29:475) [11] Kurz W, Fisher D J. Fundamentals of Solidification, Switzerland-Germany-UK-USA, Trans Tech Publications, 1989: 305 [12] Lin X, Li Y M, Liu Z X, Li T, Huang W D. Sci Technol Adv Mater, 2001; 2: 293 [13] Huang W D, Lin X, Wang M, Shen S J, Su Y P, Liu Z X. Sci Chin, 2002; 45E: 458 [14] Aziz M J. J Appl Phys, 1982; 53: 1158 [15] Jackson K A , Hunt J D. Trans Metall Soc AIME, 1996; 236: 1129 [16] Massalski T B. Binary Alloy Phase Diagram, Metals Park OH: American Society for Metals, 1986: 337 [17] Liu H Y, Jones H. Acta Metall Mater, 1992; 40: 229 [18] Cahn R W, Haasen P. Physical Metallurgy (4th edn), North-Holland: Amsterdam, 1996: 70 [19] Liu Z X, Huang W D, Yang S. Chin J Nonferrous Met, 2002; 12: 458(刘振侠,黄卫东,杨森.中国有色金属学报,2002;12:458) [20] Wang M, Lin X, Su Y P, Shen S J, Huang W D. ActaMetall Sin, 2002; 38: 337(王猛,林鑫,苏云鹏,沈淑娟,黄卫东.金属学报,2002;38:337) [21] Mullins W W, Sekerka R F. J Appl Phya, 1963; 34: 323 [22] Su Y P, Wang M, Lin X, Shen S J, Huang W D. Chin JNonferrous Met, 2003; 13: 1092 [23] Trivedi R, Kurz W. Int Mater Rev, 1994; 3949 [24] Yang S, Su Y P, Liu W J, Huang W D, Zhou Y H. ActaPhys Sin, 2003; 1: 81(杨森,苏云鹏,刘文今,黄卫东,周尧和.物理学报,2003;1:81) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|