| 钢铁生产流程的铁流对铁资源效率的影响 |
| 戴铁军;陆钟武 |
| (东北大学材料与冶金学院; 沈阳110004) |
|
| THE INFLUENCE OF IRON--FLOW IN STEEL PRODUCTION PROCESS ON ITS IRON RESOURCE EFFICIENCY |
| DAI Tiejun; LU Zhongwu |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110004 |
引用本文:
戴铁军; 陆钟武 . 钢铁生产流程的铁流对铁资源效率的影响[J]. 金属学报, 2004, 40(11): 1127-1132 .
,
.
THE INFLUENCE OF IRON--FLOW IN STEEL PRODUCTION PROCESS ON ITS IRON RESOURCE EFFICIENCY[J]. Acta Metall Sin, 2004, 40(11): 1127-1132 .
[1] Lu Z W, Cai J J, Yu Q B, Xie A G. Acta Metall Sin, 2000; 36(4) : 370(陆钟武,蔡九菊,于庆波,谢安国.金属学报, 2000;36(4) 370) [2] Guo P Z. Study of Sustainable Development for China's Industry. Beijing: Economy Science Press, 2002: 277(郭培章.中国工业可持续发展研究.北京:经济科学出版社,2002:277) [3] Kleijn R. J Ind Ecol, 2000; 3(2&3) : 8 [4] Graedel T E, Allenby B R. Industrial Ecology, New Jersey: Prentice Hall, 2003: 137 [5] Erkman S. Industrial Ecology. Beijing: Economy Daily Press, 1999: 132(Erkman S.工业生态学.北京:经济日报出版社,1999:132) [6] Lu Z W. Acta Metall Sin, 2000; 36(7) : 728(陆钟武.金属学报,2000;36(7) :728) [7] Lu Z W. Iron and Steel, 2002; 37(4) : 66(陆钟武.钢铁,2002;37(4) :66)V |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|