| 用人工神经网络模型预测钢的奥氏体形成温度 |
| 由 伟; 白秉哲; 方鸿生; 谢锡善 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| ARTIFICIAL NEURAL NETWORK APPLIED TO AUSTENITE FORMATION TEMPERATURES PREDICTION |
| YOU Wei; BAI Bingzhe; FANG Hongsheng; XIE Xishan |
| School of Materials Science and Engineering; University of Science and Technology Beijing;Beijing 100083 |
引用本文:
由伟; 白秉哲; 方鸿生 ; 谢锡善 . 用人工神经网络模型预测钢的奥氏体形成温度[J]. 金属学报, 2004, 40(11): 1133-1137 .
,
,
,
.
ARTIFICIAL NEURAL NETWORK APPLIED TO AUSTENITE FORMATION TEMPERATURES PREDICTION[J]. Acta Metall Sin, 2004, 40(11): 1133-1137 .
[1] Andrews K W. J Iron Steel Inst. 1965; 203: 721 [2] Hecht-Nielsen R. Neurocomputing, Reading, MA: Addi-son Wesley Publishing Co. Inc., 1991: 59 [3] The No.1 Iron Factory, Benxi Iron and Steel Corporation and Tsinghua University: The Atlas of Super-Cooling Austenite Transformation Diagrams, Benxi: The No.l Iron Factory Press, Benxi Iron and Steel Corporation, 1978: 1(本溪钠铁公司第一炼钢厂,清华大学机械系金属材料教研组:钢的过冷奥氏体转变曲线,本溪:本溪钢铁公司第一炼钢厂出版,1978:1) [4] American Society for Metals: Atlas of Isothermal Trans-formation and Cooling Transformation Diagrams, Metals Park, Ohio: American Society for Metals Press, 1977: 414 [5] Zhang S Z. Atlas of Super-cooling Austenite Transformation Diagrams, Beijing: Metallurgical Industry Press, 1993: 22(张世中.钢的过冷奥氏体转变曲线图集,北京:冶金工业出版社,1993:22) [6] Ha,erbin Research Institute of Welding, Machinery & Electronical Industry Ministry. CCT Atlas of Welding of Low Alloy Steels, Beijing: China Machine Press, 1990: 3(机械电子工业部哈尔滨焊接研究所.国产低合金钢焊接CCT图册,北京:机械工业出版社, 1990:3) [7] Japan Society for Irons & Steels. Atlas of CCT of Welding Steels, Tokyo: Japan Society for Iron & Steels Press, 1992: 32(日本钢铁协会.焊接用钢CCT图集,东京:日本金属学会出版社, 1992:32) [8] Japan Society for Irons & Steels. Atlas of Continuous Cooling Transformation Diagrams of Low Carbon Steels, Tokyo: Japan Society for Irons & Steels Press, 1992: 33(日本钢铁会.低碳钢连续冷却转变图集,东京:日本金属学会出版社,1992:33) [9] So S S, Karplus M. J Med Chem, 1996; 39(7) : 1524 [10] Cybenko G. Mathematics of Control, Signals and Systems, 2nd ed, New York: Springer International Press, 1980: 303 [11] Hornik K, Baldi P. Neural Network, 1989; 2: 359 [12] Chen T P, Chen H, Liu R W. IEEE Trans NN, 1995; 6(1) :25 [13] Scarselli F, Tsoi A C. Neural Networks, 1998; 11(1) : 15 [14] Vermeulen W G, Morris P F, De Weijer A P, van der Zwaag S. Ironmaking and Steelmaking, 1996; 23(5) : 433 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|