| 循环变形铜单晶体的滞后回线形状变化与驻留滑移带的萌生 |
| 李小武 王中光 李守新 |
| 中国科学院金属研究所材料疲劳与断裂国家重点实验室; 沈阳 110015 |
|
引用本文:
李小武; 王中光; 李守新 . 循环变形铜单晶体的滞后回线形状变化与驻留滑移带的萌生[J]. 金属学报, 1999, 35(6): 594-599 .
[1]Mughrabi H. Mat。, Set Eng, 1978; 33: 207 [2]Basinski Z S, Basinski S J. Prog Mater Sci, 1992; 36: 89 [3]Suresh S.Fatigue of Materials .London:Cambridge Univer sity Press, 1998: 45 [4]Jin N Y. Acta Metall, 1989; 37: 2055 [5]Polak J, Helesic J, Obrlik. Mate, Sci Eng, 1988; A101: 7 [6]Gong B, Wans Z R, Wang Z G. Mater Sci Eny; 1996; 210A: 94 [7]Lepisto T K, Kettunen P O. Mote, Sci Eng, 1986; 83: 1 [8]Gong B, Wang Z R, Wang Z G. Acta Mater, 1997; 45: 1365 [9]Li X W, Wang Z G, Sun S G, Wu S D, Li S X, Li G Y. Acta Metal Sin, 1998; 34: 545 (李小武,王中光,孙宁光,吴世丁,李守新,李广义.金属学报, 1998;34:545) [10]Hu Y M,Wang Z G.J Mater Sci Lett,1997; 16:500 [11]Li X W, Wang Z G, Li G Y, Wu S D, Li S X. Acta Mater, 1998;46:4497 [12]Li X W, Wans Z G, Li S X. Moter Sci Eng, 1999; A260: 132 [13]Li X W, Wang Z G, Li S X. Mater Sci Eng, 1999; in press [14]Li X W, Wang Z G, Li S X. Mate, Sci Eng, 1999; to be published [15]Li X W; Wang Z G,Li S X. Phios Mag Lett, 1999;in press [16]Wang R H, Mughrabi H. Mote, Sci Eng, 1984; 63: 147W |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|