| 水分子在Au和Cu及其合金表面的吸附与分解DFT计算研究* |
蒋宗佑1,2,赵宗彦1,2( ) |
1 昆明理工大学材料科学与工程学院, 昆明 650093 2 云南大学材料科学与工程学院云南省微纳材料与技术重点实验室, 昆明 650504 |
|
| STUDY ON ADSORPTION AND DISSOCIATION OF WATER MOLECULE ON Au, Cu AND THEIR ALLOYS' SURFACES BY DFT CALCULATIONS |
Zongyou JIANG1,2,Zongyan ZHAO1,2( ) |
1 School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China 2 Yunnan Key Laboratory of Micro/Nano Materials & Technology, School of Materials Science and Engineering, Yunnan University, Kunming 650504, China; |
引用本文:
蒋宗佑,赵宗彦. 水分子在Au和Cu及其合金表面的吸附与分解DFT计算研究*[J]. 金属学报, 2016, 52(12): 1586-1594.
Zongyou JIANG,
Zongyan ZHAO.
STUDY ON ADSORPTION AND DISSOCIATION OF WATER MOLECULE ON Au, Cu AND THEIR ALLOYS' SURFACES BY DFT CALCULATIONS[J]. Acta Metall Sin, 2016, 52(12): 1586-1594.
| [1] | Benton A F, Elgin J C.J Am Chem Soc, 1926; 48: 3027 | | [2] | Hutchings G J.J Catal, 1985; 96: 292 | | [3] | Haruta M, Kobayashi T, Sano H, Yamada N.Chem Lett, 1987; 16: 405 | | [4] | Haruta M, Yamada N, Kobayashi T, Iijima S.J Catal, 1989; 115: 301 | | [5] | Friend C M, Hashmi A S K.Accounts Chem Res, 2014; 47: 729 | | [6] | Wu C Y, Horibe T, Jacobsen C B, Toste F D.Nature, 2015; 517: 449 | | [7] | Qiao B T, Lin J, Wang A Q, Chen Y, Zhang T, Liu J Y.Chin J Catal, 2015; 36: 1505 | | [7] | (乔波涛, 林坚, 王爱琴, 陈洋, 张涛, 刘景月. 催化学报, 2015; 36: 1505) | | [8] | Dai W J, Yan J Q, Dai K, Li L D, Guan N J. Chin J Catal, 2015; 36: 1968 | | [8] | (代卫炯, 闫俊青, 戴珂, 李兰冬, 关乃佳. 催化学报, 2015; 36: 1968) | | [9] | Du C, Gao X H, Chen W.Chin J Catal, 2016; 37: 1049(杜诚, 高小惠, 陈卫. 催化学报, 2016; 37: 1049) | | [10] | Wang J, Cui D M.Chin J Org Chem, 2016; 36: 1163(王剑, 崔冬梅. 有机化学, 2016; 36: 1163) | | [11] | Yan K, Liao J Y, Wu X, Xie X N.RSC Adv, 2013; 3: 3853 | | [12] | Konkolewicz D, Schr?der K, Buback J, Bernhard S, Matyjaszewski K.ACS Macro Lett, 2012; 1: 1219 | | [13] | Ullmann F, Bielecki J.Ber Deutsch Chem Ges, 1901; 34: 2174 | | [14] | Nadler R, Sanz J F.J Mol Model, 2012; 18: 2433 | | [15] | Shao L, Wang Y H, Zhang D Y, Xu J, Hu X P.Angew Chem Int Ed, 2016; 55: 5014 | | [16] | Li J Y, Peng J J, Bai Y, Hu Y Q, Zhang G D, Lai G Q.Chin J Org Chem, 2009; 29: 1938 | | [16] | (厉嘉云, 彭家建, 白赢, 胡应乾, 张国栋, 来国桥. 有机化学, 2009; 29: 1938) | | [17] | Manthiram K, Beberwyck B J, Alivisatos A P.J Am Chem Soc, 2014; 136: 13319 | | [18] | Kundu J, Pradhan D.ACS Appl Mater Interfaces, 2014; 6: 1823 | | [19] | Xi Z F.Sci China. 2009; 39B: 1115(席振峰. 中国科学, 2009; 39B: 1115) | | [20] | Fiorenza R, Crisafulli C, Condorelli G G, Lupo F, Scirè S.Catal Lett, 2015; 145: 1691 | | [21] | Li L C, Wang C S, Ma X X, Yang Z H, Lu X H.Chin J Catal, 2012; 33: 1778) | | [21] | (李力成, 王昌松, 马璇璇, 杨祝红, 陆小华. 催化学报, 2012; 33: 1778) | | [22] | Kunimoto M, Nakai H, Homma T.ECS Trans, 2014; 58: 73 | | [23] | Liu T H, Zhang Z J, Fu B, Yang X M, Zhang D H.Chem Sci, 2016; 7: 1840 | | [24] | Nie X W, Luo W J, Janik M J, Asthagiri A.J Catal, 2014; 312: 108 | | [25] | Sansa M, Dhouib A, Guesmi H. J Chem Phys, 2014; 141: 064709 | | [26] | Zhang N L, Chen X, Lu Y J, An L, Li X, Xia D.Small, 2014; 10: 2662 |
|
|