| 包晶反应产物侧向生长速度的研究 |
| 常国威,金光灿,陈淑英,李青春,岳旭东 |
| 辽宁工业大学材料科学与工程学院 ,锦州 121001 |
|
| STUDY ON LATERAL GROWTH RATE OF PERITECTIC REACTION PRODUCTS |
| CHANG Guowei, JIN Guangcan, CHEN Shuying, LI Qingchun, YUE Xudong |
| School of Materials Science and Engineering, Liaoning University of Technology, Jinzhou 121001 |
引用本文:
常国威 金光灿 陈淑英 李青春 岳旭东. 包晶反应产物侧向生长速度的研究[J]. 金属学报, 2011, 47(3): 380-384.
,
,
,
,
.
STUDY ON LATERAL GROWTH RATE OF PERITECTIC REACTION PRODUCTS[J]. Acta Metall Sin, 2011, 47(3): 380-384.
| [1] Trivedi R. Acta Metall, 1970; 18: 287[2] Bosze W P, Trivedi R. Metall Mater Trans, 1974; 5B: 511[3] Fredriksson H, Nyl´en T. Met Sci, 1982; 16: 283[4] Shibata H, Arai Y, Suzuki M, Emi T. Metall Mater Trans, 2000; 31B: 981[5] Mcdonald N J, Sridhar S. Metall Mater Trans, 2003; 34A: 1931[6] Arai Y, Emi T, Fredriksson H, Shibata H. Metall Mater Trans, 2005; 36A: 3065[7] Kerr H W, Cisse J, Bolling G F. Acta Metall, 1974; 22: 677[8] Hillert M. Solidification and Casting of Metals. London: The Metals Society, 1979: 81[9] Jackson K A. Liquid Melts and Solidification. Cleveland: American Society Melts, 1958: 174[10] Jackson K A. J Cryst Growth, 1968; 3–4: 507[11] Mullins W W, Sekerka R F. J Appl Phys, 1964; 35: 444[12] Langr J S, Muller–Krumbahaar H. Acta Metall, 1978; 26: 1681[13] Trivedi R, Somboonsuk K. Acta Metall, 1985; 33: 1061[14] Trivedi R, Kurz W. Acta Metall Mater, 1994; 42: 15[15] Burton J A, Prim R C, Slichter W P. J Chem Phys, 1953; 21: 1987[16] Coriell S R, Paker R L. J Appl Phys, 1965; 36: 632[17] Jackson K A, Gilmer G H, Temkin D E, Weinberg J D, Beatty K M. J Cryst Growth, 1993; 128: 127[18] Jackson K A, Gilmer G H, Temkin D E. Phys Rev Lett, 1995; 75: 2530[19] Jackson K A, Gilmer G H, Temkin D E, Weinberg J D, Beatty K M. J Cryst Growth, 1996; 163: 461[20] Beatty K M, Jackson K A. J Cryst Growth, 1997; 174: 28[21] Jackson K A. J Cryst Growth, 1999; 198/199: 1[22] Bentz D N, Betush W J, Jackson K A. J Cryst Growth, 2003; 250: 162[23] Bentz D N, Betush W J, Jackson K A. J Cryst Growth, 2003; 250: 166[24] Poirier D R, Geiger G H. Transport Phenomena in Materials Processing. Warrendale, PA: TMS, 1994: 450[25] Kurz W, Fisher D J. Fundamentals of Solidification. Switzerland: Trans Tech Publications Ltd., 1998: 240[26] Vandyoussefi M, Kerr H W, Kurz W. Acta Mtaer, 1997; 45: 4093[27] Phelan D, Reid M, Dippenaar R. Metall Mater Trans, 2006; 37A: 985 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|