Please wait a minute...
金属学报  2010, Vol. 46 Issue (3): 380-384    DOI: 10.3724/SP.J.1037.2009.00598
  论文 本期目录 | 过刊浏览 |
DL-EPR法评价2205双相不锈钢晶间腐蚀敏感性
徐菊良; 邓博;  孙涛;  李劲; 蒋益明
复旦大学材料科学系; 上海 200433
EVALUATION OF THE SUSCEPTIBILITY TO INTERGRANULAR ATTACK OF 2205 DUPLEX STAINLESS STEEL BY DL-EPR METHOD
XU Juliang; DENG Bo; SUN Tao; LI Jin; JIANG Yiming
Department of Material Science; Fudan University; Shanghai 200433
引用本文:

徐菊良 邓博 孙涛 李劲 蒋益明. DL-EPR法评价2205双相不锈钢晶间腐蚀敏感性[J]. 金属学报, 2010, 46(3): 380-384.
. EVALUATION OF THE SUSCEPTIBILITY TO INTERGRANULAR ATTACK OF 2205 DUPLEX STAINLESS STEEL BY DL-EPR METHOD[J]. Acta Metall Sin, 2010, 46(3): 380-384.

全文: PDF(921 KB)  
摘要: 

利用Thermo-Calc软件并结合金相显微镜, 定性研究了2205双相不锈钢在800 ℃下敏化不同时间后的微观组织演变过程. 通过研究扫描速率、介质成分、介质温度和试样表面状态优化了双环电化学动电位再活化法(DL-EPR), 并用该优化方法研究了2205双相不锈钢晶间腐蚀敏感性. 结果表明: DL-EPR法能定量评价σ相对2205双相不锈钢晶间腐蚀敏感性的影响, 随敏化时间延长, σ相含量增多, 晶间腐蚀敏感性也随之增加. 腐蚀形貌的观测验证了这一规律.

关键词 : 2205双相不锈钢,  DL-EPR,  晶间腐蚀敏感性,  σ相    
Abstract:

Duplex stainless steels (DSS), consisted of ferrite and austenite, are widely used in oil, chemical, petrochemical, nuclear and marine industries because of their attractive combination of higher mechanical strength and corrosion resistance in various aggressive environments. However, precipitations of detrimental phases, such as chromium carbides, nitrides, intermetallic phases (χ, σ) inevitably occur when manufacturing conditions and welding procedure heat these duplex stainless steels to temperature ranging from 300 to 1000 ℃, which results in a reduction in corrosion properties due to the presence of chromium-depleted zones around these precipitates. In this paper, the microstructure evolution of 2205 DSS was studied qualitatively at 800 ℃ by using Thermo-Calc coupled with optical microscope. The double-loop electrochemical potentiokinetic reactivation (DL-EPR) was optimized through studying the influences caused by four factors (scan rate, temperature, the concentration of the electrolyte and the surface finish). Then the susceptibility to intergranular attack (IGA) of 2205 DSS was tested by optimized DL-EPR. The results indicated that σ phase will be precipitated in the ferrite phase when 2205 DSS aged at 800 ℃, and the volume fraction would increase with the aging time increasing. The optimized DL-EPR test can evaluate the susceptibility to IGA of 2205 DSS both quantitatively and qualitatively, which is proved by the morphologies of the sample after D--EPR test.

Key words: 2205 duplex stainless steel    DL-EPR    susceptibility to IGA    σ phase
收稿日期: 2009-09-09     
基金资助:

国家自然科学基金项目50871031和50701010, 上海市科委专项基金项目09ZR1402600和09JC1401600与上海市重点学科项目B113资助

作者简介: 徐菊良, 男, 1986年生, 硕士生

[1] Gao W, Luo J M, Yang J J. Ord Mater Sci Eng, 2005; 28: 61
(高娃, 罗建民, 杨建君. 兵器材料科学与工程, 2005; 28: 61)
[2] Nilsson J O. Mater Sci Technol, 1992; 8: 685
[3] Lopez N, Cid M, Puiggali M. Corros Sci, 1999; 41: 1615
[4] Wilms M E, Gadgil V J, Krougmen J M, Ijsseling F P. Corros Sci, 1994; 36: 871
[5] Strauss B, Schottky H, Hennuber J. Anor Allgem Chem, 1930; 188: 309
[6] Huey W R. Trans Am Soc Steel Treating, 1930; 18: 1126
[7] Streicher M A. Corros Sci, 1969; 9: 53
[8] Cihal V, Desestret A, Froment M, Wagner G H. ´ Etude de Nouveaux Tests Potentiocin´etiques de Corrosion Intergranulaire des Aciers Inoxydables. ´Etude CETIM–Center de Recherches de Firminy, C.A.F.L., 1969: 958
[9] Clarke W L, Romero V M, Danko J C. Corrosion, 1977; 77: 130
[10] Umemura F, Kawamoto T, Gijutsu B. Corr Eng Jpn, 1979; 28: 24
[11] Jin W S, Lang Y P, Rong F, Sun L J. J Chin Soc Corros Prot, 2007; 27: 54
(金维松, 郎宇平, 荣凡, 孙力军. 中国腐蚀与防护学报, 2007; 27: 54)

[12] Scully J R, Kelly R G. Corrosion, 1986; 42: 537
[13] Duret-Thual D, Bonis M, Crolet J L. Mater Corros, 2001; 52: 37
[14] Amadou T, Braham C, Sidhom H. Metall Mater Trans, 2004; 35A: 3499
[15] Garc´?a C, Mart´?n F, Blanco Y, de Tiedra M P, Aparicio M L. Corros Sci, 2009; 51: 76
[16] Deng B, Jiang Y M, Xu J L, Sun T, Gao J,Zhang L H, Zhang W, Li J. Corros Sci, 2009, doi:
10.1016/j.corsci.2009.11.020
[17] Li S S. Corros Sci Technol Prot, 2000; 12: 288
(李神速. 腐蚀科学与防护技术, 2000; 12: 288)

[18] Lee K M, Cho H S, Choi D C. J Alloys Compd, 1999; 285: 156
[19] Majidi A P, Streicher M A. Corrosion, 1984; 40: 393
[20] Sahlaoui H, Makhlouf K, Sidhom H, Philibert J. Mater Sci Eng, 2004; A372: 98

[1] 王永强,韩军,杨滨,武焕春,王西涛. 核电站主管道Z3CN20.09M不锈钢中金属间相的析出行为[J]. 金属学报, 2013, 29(4): 415-420.
[2] 梁田 康秀红 胡小强 李殿中 . 核电叶轮用双相不锈钢热处理工艺研究[J]. 金属学报, 2011, 47(7): 921-926.