| 粘土质耐火材料制品中莫来石的定量分析 |
| 叶复汗 |
| 中国科学院金属研究所 |
|
| DETERMINATION OF MULLITE IN CLAY REFRACTORY PRODUCTS |
| YEH FU-HAN Institute of Metal Research;Academia Sinica |
引用本文:
叶复汗. 粘土质耐火材料制品中莫来石的定量分析[J]. 金属学报, 1956, 1(4): 401-405.
.
DETERMINATION OF MULLITE IN CLAY REFRACTORY PRODUCTS[J]. Acta Metall Sin, 1956, 1(4): 401-405.
[1] Bowen与Greig,J.Amer.Ceram.Soc.7,238,1924, [2] 吉冈藤作与机松岭造,窑协,[38] ,200,1930. [3] 吉冈藤作,窑协,[38] ,148,1930. [4] C.W.Parmelee与Antonic R.Rodriguez,J.Amer.Ceram,Soc.25. 1,1942. [5] 秋山桂一与角川丰久,窑协,[51] ,19,1943. [6] Rieke,Ber.Deut.Keram.Ges.,11,427,1930. [7] (?)与(?)1,23,1951. 及4,181,1955. [8] (?),同上,11,507,1952.7 |
|