| 金属在范性形变后的各向异性问题 在多晶体金属中测定各向异性程度的方法 |
| W.Truszkowski |
| 波兰科学院金属研究所 |
|
| No Author |
引用本文:
W.Truszkowski. 金属在范性形变后的各向异性问题 在多晶体金属中测定各向异性程度的方法[J]. 金属学报, 1959, 4(2): 127-131.
.
[J]. Acta Metall Sin, 1959, 4(2): 127-131.
[ 1 ] W. Boas, J. K. MQckenzie: PrOgress in Meta1 Physics, 2, 90. 1950. [ 2 ] C. S. BaIrett: Structure of Meta1s, l952. [ 3 J H. W. Brownsdon: Journal of the Institute of Metals, 60, 178. l937. [ 4] I. D. Jevons: Journa1 of the Illstitute of Meta1s, 60. 174, 1937. [ 51 W. M. Baldwin: Meta1s Technology, Tech. Pub. 1455, April, 1942. [ 6] A. Krupkowski, S. Kawil'1ski: Journal of the Institute of Metal3, 75. 869. 19so: N Hutnik l6, 347, 19'0. [ 71 A. Krupkowski, A. B1ock-Bolten: Prace Instytutu Mechaniki, Z. 7. 34, 1953. [ 81 W. Truszkowski: Archiwum Hutnictwa, 1, 171. 1956 |
|