摘要: 本文叙述了国内外已建立的各种类型连续铸锭机的优缺点,讨论了各项主要设备的合理设计和应用对于浇铸凝固过程和铸坯质量的影响。关于改善铸坯质量和防止浇铸过程铸坏发生断裂的各种方法,也作了扼要的介绍。
Abstract:In the present paper, various types of continuous casting machines employed in steelworksare described. Design and operation of such machines are discussed and suggestions for propermeasures to improve the quality of casting billets are reviewed.
收稿日期: 1959-04-18     
[1] #12.
[2]#12.
[3]#12.
[4] #12.
[5] #12.
[6] #12.
[7] #12.
[8] #12.
[9] #12.
[10] #12.
[11] J. Savage and W. H. Pritchard: Continuous casting of rupture of the billet, Iron & Steel. 27. 1954, 649--653.
[12] The freezing of continuous cast steel, Metal Treatment and Drop Forging, 17, 1959, 3--10.
[13] A. G. Grimshaw and B. O. Smith: A pneumatic level indicator for the continuous casting process, J. I. S. I., 185, 1957, 235--237.
[14] G. Fenton and J. Pearson: Continuous casting on the B.I.S.R.A. experimental plant, J.I.S.I., 189, 1958. 160--167.
[15] H. Krainer and B. Tarmann: New experience in the continuous casting of steel. J.I.S.I., 190, 1958. 105--111.
[16] K. G. Speith: Continuous casting of steel in western Germany, J.I.S.I., 190, 1958, 158--161.
[17] B. H. C. Waters: Continuous casting of high-speed steel, J.I.S.I., 190, 1958, 233--248.
[18] M. Tenenbaum, C. T. Schrader and L. Mair: Solidification characteristics of continuously cast lowcarbon steels, J.I.S.I., 191, 1958, 20--33.
[19] K. G. Speith und A. Bungeroth: Das Stranggiessen von Stahl nach dem Junghans-Verfahren, Stahl und Eisen, 72, 1952, 869--885.
[20] J. Savage: Application of continuous casting to steel, Metal Treatment & Drop Forging, 22. 1955, 277--87.
[21] ABC生钢连续铸造展望(1-4) ,电气制钢,vol.290,1958,No.3. p.209-19;No.4,p.296-307;No.5,p.379-385;No.6,p.457-468.
[22] 东工炼钢教研组:连续铸钢,冶金译述,1956. 6.
[23] 徐宝陞:连续铸钢装置的合理设计,钢铁,1959年14期621页.
[24] 倾斜式连续铸锭研究(一),冶金部大连钢厂、中国科学院金属研究所、第一机械工业部重型与矿山机械研究所,1959年./
No related articles found!