| 钢的连续铸锭 |
| 赵惠田;张顺南 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| A GENERAL REVIEW ON CONTINUOUS CASTING OF STEEL |
| CHAO HWEI-TIAN;CHANG SHUN-NAN Institute of Metal Research; Academia Sinica |
引用本文:
赵惠田;张顺南. 钢的连续铸锭[J]. 金属学报, 1959, 4(4): 333-350.
,
.
A GENERAL REVIEW ON CONTINUOUS CASTING OF STEEL[J]. Acta Metall Sin, 1959, 4(4): 333-350.
[1] #12. [2]#12. [3]#12. [4] #12. [5] #12. [6] #12. [7] #12. [8] #12. [9] #12. [10] #12. [11] J. Savage and W. H. Pritchard: Continuous casting of rupture of the billet, Iron & Steel. 27. 1954, 649--653. [12] The freezing of continuous cast steel, Metal Treatment and Drop Forging, 17, 1959, 3--10. [13] A. G. Grimshaw and B. O. Smith: A pneumatic level indicator for the continuous casting process, J. I. S. I., 185, 1957, 235--237. [14] G. Fenton and J. Pearson: Continuous casting on the B.I.S.R.A. experimental plant, J.I.S.I., 189, 1958. 160--167. [15] H. Krainer and B. Tarmann: New experience in the continuous casting of steel. J.I.S.I., 190, 1958. 105--111. [16] K. G. Speith: Continuous casting of steel in western Germany, J.I.S.I., 190, 1958, 158--161. [17] B. H. C. Waters: Continuous casting of high-speed steel, J.I.S.I., 190, 1958, 233--248. [18] M. Tenenbaum, C. T. Schrader and L. Mair: Solidification characteristics of continuously cast lowcarbon steels, J.I.S.I., 191, 1958, 20--33. [19] K. G. Speith und A. Bungeroth: Das Stranggiessen von Stahl nach dem Junghans-Verfahren, Stahl und Eisen, 72, 1952, 869--885. [20] J. Savage: Application of continuous casting to steel, Metal Treatment & Drop Forging, 22. 1955, 277--87. [21] ABC生钢连续铸造展望(1-4) ,电气制钢,vol.290,1958,No.3. p.209-19;No.4,p.296-307;No.5,p.379-385;No.6,p.457-468. [22] 东工炼钢教研组:连续铸钢,冶金译述,1956. 6. [23] 徐宝陞:连续铸钢装置的合理设计,钢铁,1959年14期621页. [24] 倾斜式连续铸锭研究(一),冶金部大连钢厂、中国科学院金属研究所、第一机械工业部重型与矿山机械研究所,1959年./ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|