| 纯铁中稀土夹杂物形态的研究 |
| 李静媛 |
| 中国科学院金属研究所 |
|
| THE MORPHOLOGY OF INCLUSIONS IN PURE IRON CONTAINING RARE EARTH METALS |
| LEE CHING-YUAN Institute of Metal Research;Academia Sinica |
引用本文:
李静媛. 纯铁中稀土夹杂物形态的研究[J]. 金属学报, 1963, 6(2): 146-190.
.
THE MORPHOLOGY OF INCLUSIONS IN PURE IRON CONTAINING RARE EARTH METALS[J]. Acta Metall Sin, 1963, 6(2): 146-190.
[1] Howard,O.B.:Metal Progr.,1954,66(4) ,115. [2] Post,C.B.,Schoffstall,D.G.,Beaver,H.O.:J.Metals,1951,3,973. [3] Post,C.B.,Beaver,H.O.:Blast Furnace Steel Plant,1953,41,627. [4] Perkins,R.A.,Binder,W.O.:J.Metals,1957,9,239. [5] Henke,R.H.,Lula,R.A.:J.Metals,1954,6,883. [6] Russell,J.V.:J.Metals,1954,6,438. [7] Morrogh,H.,Williams,N.J.:J.Iron Steel Inst.,1948,158,306. [8] Evans,H.:Iron Steel,1954,27,567. [9] Lillieqvist,G.A.,Mickelson,C.G.:Elec.Furnace Steel Proc.,1952,10,117. [10] DuMont,C.S.,Gates,J.E.,Henderson,C.M.:Trans.Am.Soc.Metals,1956,48,306. [11] Sims,C.E.:Trans.AIME,1959,215,367. [12] Geller,S.,Wood,E.A.:Acta Cryst.,1956,9,563. [13] Zachariasen,W.H.:Acta Cryst.,1949,2,57. [14] Zachariasen,W.H.:Acta Cryst.,1948,1,265. [15] Zachariasen,W.H.:Acta Cryst.,1949,2,60. [16] Geller,S.:J.Chem.Phys.,1956,24,1236. [17] Bevan,D.J.M.:J.Inorg.Nucl.Chem.,1955,1,49. [18] Keith,M.L.,Roy,R.:Am.Mineralogist,1954,39,1. [19] Wold,A.,Word,R.:J.Am.Chem.Soc.,1954,76,1029. [20] Eastman,E.D.:J.Am.Chem.Soc.,1951,73,3896. [21] Pitha,J.J.,Smith,A.L.:J.Am.Chem.Soc.,1947,69,1870. [22] Gilles,P.W.,Eastman,E.D.,Bromloy,L.A.:J.Am.Chem.Soc.,1950,72,2248. [23] Banks,E.,Stripp,K.F.,Newkirk,H.W.,Ward,R.:J.Am.Chem.Soc.,1952,74,2450. [24] Harwood,M.G.:Proc.Phys.Soc.(London),1955,B68,586. [25] Moruzzi,V.L.,Shafer,M.W.:J.Am.Ceram.Soc.,1960,43(7) ,367. [26] Fischer,W.A.,Wahlster,M.:Arch.Eisenhüttenw.,1958,1. [27] #12 [28] Mauguin,M.C.:Compt.Rend.,1956,243,1220. [29] Picon,M.M.:Compt.Rend.,1956,243,1769. [30] Flahaut,M.J.:Compt.Rend.,1956,242,1318. [31] Picon,M.M.:Compt.Rend.,1956,242,1321. [32] Picon,M.M.:Compt.Rend.,1956,242,516. [33] Flahaut,M.J.:Compt.Rend.,1955,241,1775. [34] #12 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|