| 某含铜钴土矿两段硫酸化焙烧过程 |
| 谭庆麟;王永禄 |
| 中国科学院贵金属研究所;中国科学院贵金属研究所 |
|
| STUDIES ON THE TWO-STAGE SULPHATING ROASTING PROCESS |
| TAN CHING-LIN; WANG YUNG-LU(Institute of Preciou Metals; Academia Sinica) |
引用本文:
谭庆麟;王永禄. 某含铜钴土矿两段硫酸化焙烧过程[J]. 金属学报, 1964, 7(2): 136-144.
,
.
STUDIES ON THE TWO-STAGE SULPHATING ROASTING PROCESS[J]. Acta Metall Sin, 1964, 7(2): 136-144.
[1] #12 [2]#12 [3] #12 [4] #12 [5] Kellogg, H. H.: J. Metals, 1956, 8, 1105. [6] Thornhill, P. G., Pidgeon, L. M.: J. Metals, 1957, 9, 989. [7] 譚庆麟、王永祿、段維垣等:某低品位含銅鈷土矿的处理,1960年中国科学院技术科学部于昆明召开的会議論文。 [8] 苏鑑、段維垣等:某地含銅鈷土矿两段硫酸化焙烧半工业性試驗报告,1962年云南省金属学会年会論文. [9] Hodgman, C. D.: Handbook of Chemistry and Physics, 39th ed., (Chemical Rubber Publishing Co, Cleveland, Ohio, 1957--1958) . [10] Mellor, J. W.: A Comprehensive Treatise on Inorganic and Theoretical Chemistry, 1935, vol. 14, p. 761, 310. |
|