| 锰-铝合金系中铁磁性ζ相的磁畴结构 |
| 曽训一 |
| 中国科学院冶金研究所 |
|
| DOMAIN STRUCTURE OF FERROMAGNETIC ζ-PHASE IN Mn-Al SYSTEM |
| TSENG HSUN-YI (Institute of Mctallurgy; Academia Sinica) |
引用本文:
曽训一. 锰-铝合金系中铁磁性ζ相的磁畴结构[J]. 金属学报, 1964, 7(2): 174-178.
.
DOMAIN STRUCTURE OF FERROMAGNETIC ζ-PHASE IN Mn-Al SYSTEM[J]. Acta Metall Sin, 1964, 7(2): 174-178.
[1] Kono. H.: J. Phys. Soc. Japan, 1958, 13, 1444. [2] Koster, W., Wachtel, E.: Z. Metallk., 1960, 51, 271. [3] Koch, A. J. J., Hokkeling, P., V. D. Steeg, M. G. et al.: J. Appl. Phys., 1960, 31, 75s. [4] Bohlmann, M. A.: J. Appl. Phys., 1962, 33, 1315. [5] #12 [6] Hall, E. O.: Proc. Phys. Soc. (London), 1957, B70, 254. [7] Elmore, W. C.: Phys. Rev., 1938, 54, 309. 近角聪信、鈴木賢造:金属物理,1956,2,207. [8] Elmore, W. C.: Phys. Rev., 1938, 53, 757. Roberts, B. W., Bean, C. P.: Phys. Rev., 1954, 96, 1494. Perthel, R., Andra, W.: Ann. Phys. (Lipiz), 1957, 19, 265. [9] Kittel, C., Galt, J. K.: Solid State Phys., 1956, 3, 439. [10] Williams, H. J., Bozorth, R. M., Shockley, W.: Phys Rev., 1949, 75, 155. [11] Goodenough, J. B.: Phys. Rev., 1956, 102, 356. [12] #12 [13] #12 [14] Campbell, R. B., Julien, C. A.: J. Appl. Phys., 1961, 32, 346s. [15] Landau, L., Lifshitz, E.: Phys. Z. Sowjet., 1935, 8, 153. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|