| 铁-锰、铝系奥氏体钢——耐热钢、无磁钢和低温钢 |
| 张彦生;师昌绪 |
|
| A STUDY ON Fe-Mn-Al AUSTENITIC STEELS |
| CHANG YEN-SHENG; SHIH CHANG-HSU |
引用本文:
张彦生;师昌绪. 铁-锰、铝系奥氏体钢——耐热钢、无磁钢和低温钢[J]. 金属学报, 1964, 7(3): 285-300.
,
.
A STUDY ON Fe-Mn-Al AUSTENITIC STEELS[J]. Acta Metall Sin, 1964, 7(3): 285-300.
[1] Koster, W., Tonn, W.: Arch. Eisenhuttenw., 1933-1934, 365. [2] Schmatz, D. J.: Trans. AIME, 1959, 215, 113. [3] Hansen, M., Anderk, A.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) , p. 90, 527, 668, 713, 725, 730, 734. [4] Thielemann, R. H.: Proc. Am. Soc. Testing Mater., 1940, 46, 788. [5] Brown, J. T.: Metal Progr., 1958, 74, (11) , 87. [6] 郭蘊宜等:待发表. [7] Kubaschewski, O., Hopkins, B. E.: Oxidation of Metal and Alloys, (Butterworths, 1953) , p. 267. [8] Brick, R. M., Low, J. R., Lorig, C. H.: Behavior of Metals at Low Temperature, (ASM. 1953) p. 98-100 |
|