| 镍基高温合金的强化 |
| 颜鸣皋;陈学印 |
|
| ON THE STRENGTHENING OF NICKEL-BASE SUPERALLOYS |
| YEN MING-KAO; CHEN HSUEH-YING |
引用本文:
颜鸣皋;陈学印. 镍基高温合金的强化[J]. 金属学报, 1964, 7(3): 307-321.
,
.
ON THE STRENGTHENING OF NICKEL-BASE SUPERALLOYS[J]. Acta Metall Sin, 1964, 7(3): 307-321.
[1] Betteridge, W.: The Nimonic Alloys, (Edward Arnold, 1959) . [2] Ver Snyder, F. L.: High Temperature Materials, Conference Held in Cleveland, Ohio, ed. R. F. Hehemann, (AIME, 1959) , p. 3. [3] #12 [4] Bieber, C. G., Raudebaugh, R. J.: Precipitation from Solid Solution, (ASM, 1959) , p. 417. [5] #12 [6] Betteridge, W.: Metallurgia, 1961, 63, 79. [7] Jahnke, L. P., Frank, R. G.: Metal Progr., 1958, 74, (5) , 77. Jahnke, L. P., Frank, R. G.: Metal Progr., 1958, 74, (6) , 86. [8] Glenny, E.: Foundary, 1961, 111, 293. [9] Drennen, D. C., Lund, C. H.: PB, No. 161245, 1961. [10] #12 [11] Jaffee, R. I.: Progress in Metal Physics, (Pergamon, 1958) , vol. 7, p. 65. [12] #12 [13] Hansen, M.: Constitution of Binary Alloys, 2nd ed., (McGraw-Hill, 1958) . [14] #12 [15] #12 [16] Guard, R. W.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 270. [17] Fell, E. A.: Metallurgia, 1961, 63, 157. [18] Flinn, P. A.: Trans. AIME, 1960, 218, 145. [19] Guard, R.. W., Westbrook, J. H.: Trans. AIME, 1959, 215, 807. [20] Radavich, J. F., Pennington, W. J.: Metal Progr., 1961, 79, (2) , 94. [21] #12 [22] Beattie, Jr., H. J., Ver Snyder, F. L.: Trans. Am. Soc. Metals, 1957, 49, 883. [23] Kaufman, M.: Trans. AIME, 1963, 227, 405. [24] Radavich, J. F., Couts, Jr., W. H.: Trans. Am, Soc. Metals, 1961, 54, 591. [25] Radavich, J. F., Boesch, W. J.: Advance in X-ray Analysis, ed. W. M. Mueller, (Plenum Press, 1960) , vol. 4, p. 233. [26] Beattie, Jr., H. J.: Acta Cryst., 1958, 11, 607. [27] #12 [28] #12 [29] #12 [30] #12 [31] #12 [32] McLean, D.: Vancancies and Other Point Defects in Metals and Alloys, (Inst. Metals, 1958) , p. 159. [33] #12 [34] Schoeck, G.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 79. [35] Cottrell, A. H., Relation of Properties to Microstructure, (ASM, 1954) , p. 330. [36] Nutting, J., Arrowsmith, J. M.: Structural Processes in Creep, (Iron Steel Inst., 1962) , p. 147. [37] Mader, S.: Electron Microscopy and Strength of Crystals, (Interscience. 1962) , p. 183. [38] #12 [39] #12 [40] Fell, E. A., Mitchell, W. I., Wakeman, D. W.: Structural Processes in Creep, (Iron Steel Inst., 1962,), p. 136. [41] Nordheim, R., Grant, N. J.: Trans. AIME, 1954, 200, 211. [42] Wilde, R. F., Grant, N. J.: Trans. AIME, 1957, 209, 865. [43] Kaufman, M., Palty, A. E.: Trans. AIME, 1960, 218, 107. [44] Hagel, W. C., Beattie, Jr., H. J.: Trans. AIME, 1959, 215, 967. [45] Rogen, N. E., Grant, N. J.: Trans. AIME, 1960, 218, 180. [46] Mihalisin, J. R., Decker, R. F.: Trans. AIME, 1960, 218, 507. [47] #12 [48] #12 [49] Mihalisin, J. R., Carroll, K. G.: Symposium on Advance in Electron Metallography, (ASTM, 1958) , p. 68. [50] #12 [51] McLean, D.: Met. Rev., 1962, 7, (28) , 481. [52] Firey, D. N., Freeman, J. W., White, A. E.: NACA TN-No. 2385, 1951. [53] Mott, N. F., Nabarro, F. R. N.: Conference on Strength of Solid, (Bristal, 1948) , p. 1. [54] #12 [55] Nicholson, R. B., Nutting, J., Hirsch, P. B.: J. Inst. Metals, 1957-1958, 86, 7. [56] Dew-Hughes, D., Robertson, W. D.: Acta Met., 1960. 8, 147. [57] Kelly, A., Fine, M. F.: Acta Met., 1957, 5, 365. [58] Kelly, A.: Phil. Mag., 1958, 3, 1472. [59] Orowan, E.: Symposium on Internal Stresses in Metals and Alloys, (Inst. Metals, 1948) , p. 47. [60] Fischer, J. C., Hart, E. W., Pry, R. H.: Acta Met., 1953, 1, 336. [61] 张兴钤:合金的強化,全国第一次金属物理学术报告会論文,1961年,沈阳. [62] Gregory, E., Goetzel, C. G.: Trans. AIME, 1958, 212, 868. [63] Cremens, W. S., Grant, N. J.: Proc. Am. Soc. Testing Mater., 1958, 58, 714. [64] Gatti, A.: Powder Met., 1962, (10) , 77. [65] Schafer, R. J., Quatinetz, M., Weeton, J. W.: Trans. AIME, 1961, 221, 1099. [66] 师昌緒:高温材料的发展,1963年中国金属学会学术年会論文,青島. [67] Greenwald, M., Sparrow, W. H.: J. Metals, 1963, 15, 78. [68] Cottrell, A. H.: Symposium on Creep and Fracture of Metals at High Temperature, (London, 1956) , p. 141. [69] Glen, J.: J. Iron Steel Inst. (London), 1958, 189, 333. [70] Hale, K. F.: Vierter Internationaler Kongress fur Electronen Mikroskopie, (Berlin, 1958) , p. 650. [71] #12 [72] #12 [73] Betteridge, W., Franklin, A. W.: J. Inst. Metals, 1956-1957, 85, 473. [74] Weaver, C. W.: J. Inst. Metals, 1959-1960, 88, 296. [75] Fleetwood, M. J.: J. Inst. Metals, 1962, 90, 429. [76] Weaver, C. W.: J. Inst. Metals, 1962, 90, 404. [77] #12 [78] McLean, D.: Grain Boundaries in Metals, (Oxford, 1957) , p. 322. [79] McLean, D.: Mechanical Properties of Metals, (Wiley, 1962) , p. 223. [80] Cottrell, A. H.: Structural Processes in Creep, (Iron Steel Inst. 1962) , p. 1. [81] #12 [82] Davies, P. W., Dennison, J. P.: J. Inst. Metals, 1958-1959, 87, 119. [83] Chang, H. C. (张兴钤), Grant, N. J.: Trans. AIME, 1953, 197, 1175. Chang, H. C. (张兴钤), Grant, N. J.: Trans. AIME, 1956, 206, 544. [84] Gemmell, G. D., Grant, N. J.: Trans. AIME, 1957, 209, 417. [85] Resnick, R., Seigle, L.: Trans. AIME, 1957, 209, 87. [86] Chen, C. W. (陈志文), Machlin, E. S.: Trans. AIME, 1957, 209, 829. [87] Reid, B. J., Greenwood, J. N.: Trans. AIME, 1958, 212, 503. [88] Weaver, C. W.: Acta Met., 1960, 8, 343. [89] Weaver, C. W.: J. Inst. Metals, 1958, 87, 126. [90] Conrad, H.: Mechanical Behavior of Materials at Elevated Temperatures, (McGraw-Hill, 1961) , p. 218. [91] Zener, C.: Elasticity and Anelasticity of Metals, (Univ. of Chicago Press, 1948) , p. 158. [92] Gifkins, R. D.: Acta Met., 1956, 4, 98. [93] Weaver, C. W.: J. Inst. Metals, 1959-1960, 88, 296. [94] #12 [95] Pennington, W. J.: Metal Progr., 1958, 73, (3) , 82. [96] Decker, R. F., Freeman, J. W.: Trans. AIME, 1960, 218, 277. [97] McLean, D.: J. Inst. Met., 1957, 85, 468.M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|