| 钼中非金属夹杂物的鉴定 |
| 朱惠滋;李静媛;浦以健 |
|
| ON THE IDENTIFICATION OF NONMETALLIC INCLUSIONS IN MOLYBDENUM |
| CHU HUI-TZǔ; LI CHIN-YEN; P'U YI-CHIEN |
引用本文:
朱惠滋;李静媛;浦以健. 钼中非金属夹杂物的鉴定[J]. 金属学报, 1966, 9(2): 189-239.
,
,
.
ON THE IDENTIFICATION OF NONMETALLIC INCLUSIONS IN MOLYBDENUM[J]. Acta Metall Sin, 1966, 9(2): 189-239.
[1] Parke, R. M., Ham, J. L.: Trans AIME, 1947, 171, 416. [2] Few, W. E., Manning, G. K.: J. Metals, 1952, 4, 271. [3] Maringer, R. E., Schwope, A. D.: Trans. AIME, 1954, 200, 365. [4] Olds, L. E., Rengstorff, G. W.: J. Metals, 1956, 8, 150. [5] Semchyshen, M., Barr, R. Q.: PB 126447.' |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|