| 稀土球铁与稀土-镁球铁中元素的分布 |
| 韩其勇;吴卫江;方克明;卢静;张保军;谢德义;裴丽侠 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| DISTRIBUTION OF NODULARIZING ELEMENTS IN R. E. TREATED SPHEROIDAL GRAPHITE CAST IRONS |
| Han Qiyong;Wu Weijiang;Fang Keming;Lu Jing;Zhang Baojun;Xie Deyi;Pei Lixia Beijing Institute of Iron and Steel Technology |
引用本文:
韩其勇;吴卫江;方克明;卢静;张保军;谢德义;裴丽侠. 稀土球铁与稀土-镁球铁中元素的分布[J]. 金属学报, 1979, 15(1): 1-187.
,
,
,
,
,
,
.
DISTRIBUTION OF NODULARIZING ELEMENTS IN R. E. TREATED SPHEROIDAL GRAPHITE CAST IRONS[J]. Acta Metall Sin, 1979, 15(1): 1-187.
[1] Hillert, M. and Lindblom, Y., J. Iron Steel Inst., 176 (1954) , 388. [2] (1971) , № 7, 36. [3] 12 (1961) , № 2, 233. [4] Spendler, W. A. and Flinn, R. A., Trans. Amer. Foundrymen's Soc., 70 (1962) . 1017. [5] Michael, A. B., J. Iron Steel Inst., 178 (1954) , № 2, 160. [6] 20 (1965) . № 2. 236. [7] 张博,山本悟,川野丰?,尾崎良平,日本金属学会志,41(1977) ,471. [8] 奥本武臣,饭岛史郎,铸物,35(1963) ,728. [9] 饭岛史郎,奥本武臣,铸物,38(1966) ,277. [10] Olette, M., Kohn, H., and Kozakevitch, P., Fonderie, (1965) , № 229, 87. [11] 4 (1957) , № 1, 177. [12] (1965) , № 4, 30. [13] Warrick, R. J., Trans, Amer. Foundrymen's Soc., 74 (1966) , 722. [14] Jacobs, M. H., Law, T. J., Melford, D. A. and Stowell, M. J., Metals Technol., 1 (1974) , № 11, 491. [15] Pirs, J., Microstruct. Sci., 3 (1975) , Pt. A, 91. [16] Katz, L. and Penfold, A. S., Rev. Mod. Phys., 24 (1952) , 28. [17] (1960) , 55. [18] Lux, B., Cast Metals Res., 8 (1972) , № 2, 49. [19] Mcswain, R. H. and Bates, C. E., The Metallurgy of Cast Iron, 1975, p. 423.
[20] Van Rooyen, G. T. and Paul, G., Metal Sci. J., 8 (1974) , 370. [21] Minkiff, I., Joint Conference on the Solidification of Metals. Brighton, 1967, Paper №. B/111/15. ISI Publication 110, 1968. [22] Zeedijk, H. B., J. Iron Steel Inst., 203 (1965) , 737. [23] 北京钢铁学院同位素小组,待发表工作. [24] Hunter, M. J. and Chadwick, G. A., J. Iron Steel Inst., 210 (1972) , 117. [25] 张博,山本悟,川野丰,尾崎良平,日本金属学会志,41(1977) ,464. [26] 张博,山本悟,川野丰,尾崎良平,日本金属学会志,41(1977) ,564,571. [27] Sadocha, J. P. and Grazleski, J. E., The Metallurgy of Cast Iron, 1975, p. 443. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|