| 电渣重熔过程中渣池内的温度分布 |
| 傅杰;陈崇禧;陈恩普;王涌 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| TEMPERATURE DISTRIBUTION ROUND THE MOLTEN SLAG POOL IN THE PROCESS OF ELECTROSLAG REFINING |
| Fu Jie;Chen Chongxi;Chen Enpu;Wang Yong Beijing Institute of Iron and Steel Technology |
引用本文:
傅杰;陈崇禧;陈恩普;王涌. 电渣重熔过程中渣池内的温度分布[J]. 金属学报, 1979, 15(1): 44-50.
,
,
,
.
TEMPERATURE DISTRIBUTION ROUND THE MOLTEN SLAG POOL IN THE PROCESS OF ELECTROSLAG REFINING[J]. Acta Metall Sin, 1979, 15(1): 44-50.
[1] (1963) , 9. [2] Wolfenbuttel, H. M. und Hanau, M. W., Arch. Eisenhuettenw., 44 (1973) , 19. [3] Paton, B. E., et al., Int. Iron Steel Congress 1974, Vol. Ⅲ, 4, Special Metallurgical Treatment of Highgrade Steels, 4. 2. 2. 6. [4] 川上正博,铁钢,62(1976) ,117. [5] 川上正博,铁钢,63(1977) ,99. [6] Mitchell, A. et al., Electroslag Refining. The Iron and Steel Institute, London, 1973, 3. [7] Fraser, M. E. and Mitchell, A., Ironmaking Steelmaking, 3 (1976) , 279. [8] (1963) , 94.2 |
|