| 一水硬铝石-高岭石型铝土矿的选矿 |
| 李跃吾;陈东 |
| 沈阳铝镁设计院;沈阳铝镁设计院 |
|
| BENEFICIATION OF DIASPORE-KAOLINITE-BEARING BAUXITE BY FLOTATION |
| Li Yuewu;Chen Dong Shenyang Designing Institute of Aluminum and Magnesium Industry |
引用本文:
李跃吾;陈东. 一水硬铝石-高岭石型铝土矿的选矿[J]. 金属学报, 1979, 15(3): 319-322.
,
.
BENEFICIATION OF DIASPORE-KAOLINITE-BEARING BAUXITE BY FLOTATION[J]. Acta Metall Sin, 1979, 15(3): 319-322.
|