Please wait a minute...
金属学报  1979, Vol. 15 Issue (3): 351-444    
  论文 本期目录 | 过刊浏览 |
非晶态Gd-Co薄膜的结构与磁性
杨翠英;王荫君;王忠铨;李方华
中国科学院物理研究所;中国科学院物理研究所;中国科学院物理研究所;中国科学院物理研究所
CORRELATION BETWEEN STRUCTURE AND MAONETIC PROPERTIES OF AMORPHOUS Gd-Co FILMS
Yang Cuiying;Wang Yinzhong;Wang Zhongquan;Li Fanghua Institute of Physics; Academia Sinica
引用本文:

杨翠英;王荫君;王忠铨;李方华. 非晶态Gd-Co薄膜的结构与磁性[J]. 金属学报, 1979, 15(3): 351-444.
, , , . CORRELATION BETWEEN STRUCTURE AND MAONETIC PROPERTIES OF AMORPHOUS Gd-Co FILMS[J]. Acta Metall Sin, 1979, 15(3): 351-444.

全文: PDF(1276 KB)  
摘要: 本文用电子衍射方法研究了非晶态Gd-Co薄膜(400—700A)的结构,测定了五个试样的径向分布函数,并把其中两个试样的径向分布函数与它们的磁性(一为垂直膜面单轴各向异性,另一为平面各向异性)联系,发现Gd-Co薄膜的垂直膜面磁各向异性可能与膜中异类原子的最近邻配位数较大有关。
Abstract:The structure of amorphous Gd-Co films 400-700Ain thickness has been stu-died by electron diffraction and results of the radial distribution functions (RDF)have been obtained for five samples. In comparing the RDF for two of the samp-les with perpendicular and in-plane anisotropy respectively, it is shown that cor-relation between the nearest neighbour coordination of different kind of atoms inthe amorphous Gd-Co films and its magnetic anisotropy may be established.
收稿日期: 1979-03-18     
[1] Fujime, S., Jap. J. Appl. Phys., 5 (1966) , 764.
[2] Richter, H. and Steeb, S., Naturwissenschaften, 21 (1958) , 512.
[3] Ichikawa, T., Phys. Status Solidi, A19 (1973) , 347
[4] Dixmier, J. and Guinier, A., Rev. Met. (Paris), 64 (1967) , 53.
[5] Cangill, G. S. Ⅲ and Cochrane, R. W., J. Phys. (Paris), 35 (1974) , C4--269.
[6] Wagner, C. N. J., J. Vac. Sci. Technol., 6 (1969) , 650.
[7] Graczyk, J. F., AIP Conf. Proc., (1976) , № 34, 343.
[8] Nandra, S. S. and Grundy, P. J., J. Phys., F7 (1977) , 207.
[9] Wagner, C. N. J., Heiman, N., Huang, T. C. and Onton, A., AIP Conf. Proc., (1976) , № 29, 188.
[10] Cargill, G. S. Ⅲ, AIP Conf. Proc., (1974) , № 18, 631.
[11] Wright, A. C. and Better, A. J. L., Phys. Chem. Glasses, 17 (1976) , 122--145.
[12] Cargill. G. S. Ⅲ, Solid State Phys., 30 (1975) . 227.
[13] 王荫君等,物理学报,26(1977) ,187.
[14] 谢侃,郑德娟,物理(1978) ,296.
[15] Dove, D. B., Phys. Thin Films, 7 (1973) , 1.
[16] Leonhardt, R., Richter, H. und Rossteutscher, W., Z. Phys., 165 (1961) , 121.
[17] Ichikawa, T., Jap. J. Appl. Phys., 9 (1970) , 748.
[18] Gandais, M., Theye, M. L., Fisson, S. and Boissonade, J., Phys. Status Solidi, B58 (1973) , 601.
[19] 2 (1957) , 29.
[20] Chaudhari, P. and Cronemeyer, D. C., AIP Conf. Proc., (1976) , № 29, 113.
[21] 20 (1975) , 121.]
No related articles found!