| 准解理断口的特征长度参数与断裂韧度的关系 |
| 孙福玉 |
| 冶金工业部钢铁研究总院 |
|
| CORRELATION BETWEEN THE CHARACTERISTIC LENGTH PARAMETER OF THE QUASI-CLEAVAGE FRACTURE AND FRACTURE TOUGHNESS |
| Sun Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry |
引用本文:
孙福玉. 准解理断口的特征长度参数与断裂韧度的关系[J]. 金属学报, 1980, 16(1): 59-134.
.
CORRELATION BETWEEN THE CHARACTERISTIC LENGTH PARAMETER OF THE QUASI-CLEAVAGE FRACTURE AND FRACTURE TOUGHNESS[J]. Acta Metall Sin, 1980, 16(1): 59-134.
[1] Spitzig, W.A., Amer. Soc. Test. Mater., Spec. Tech. Publ. № 453, p. 90. [2] Brok, D., Eng. Fract. Mech., 6 (1974) , 173. [3] 陈篪,金属学报,13(1977) ,57. [4] 陈篪,金属断裂研究文集,冶金工业出版社,1978年,p.30. [5] Levy, N., Marcal, P.V., Ostergren, W.T. and Rice, J.R., Int. J. Fract. Mech., 7(1971) , 143. [6] Riichie, R.O., Knott, J.F. and Rice, J.R., J. Mech. Phys. Solids, 21 (1973) , 395. |
|