| 含磷深冲钢冷轧和退火板材的晶体空间取向分布 |
| 胡郇 |
| 美国钢铁公司研究所 |
|
| SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED AND IN ANNEALED SHEETS OF DEEP-DRAWING PHOSPHORUS STEEL |
| Hsun Hu U. S. Steel Research Laboratory |
引用本文:
胡郇. 含磷深冲钢冷轧和退火板材的晶体空间取向分布[J]. 金属学报, 1980, 16(2): 121-139.
.
SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED AND IN ANNEALED SHEETS OF DEEP-DRAWING PHOSPHORUS STEEL[J]. Acta Metall Sin, 1980, 16(2): 121-139.
[1] Hu, H., Texture Cryst. Sol., 2 (1976) , 113. [2] Hu, H., Met. Trans., 8A (1977) , 1567. [3] Hu, H., Texture Cryst. Sol., 3 (1979) , 215--230. [4] Hu, H., "Effect of Silicon on Annealing Texture, Plastic Anisotropy, and Mechanical Properties of Low-Carbon Phosphorus-Containing Steels," Proceedings of Symposium on Modern Developments in HSLA Formable Steels, TMS-AIME Fall Meeting, October 24--27, 1977, Chicago, Ⅰ.Ⅱ. [5] Hu, H., "Low-Carbon Phosphorus Steels for High-Strength Cold-Rolled Sheet Applications," Unpublished work, U. S. Steel Research Laboratory. [6] Roe, R. J., J. Appl. Phys., 36 (1965) , 2024. [7] Roe, R. J., J. Appl. Phys., 37 (1966) , 2069. [8] Bunge, H. J., Z. Metallk., 56 (1965) , 872. [9] Bunge, H. J., Mathematische Methoden der Texturanalyse, Akademie-Verlag, Berlin, 1969. [10] Morris, P. R. and Heckler, A. J., Advances in X-Ray Analysis, 1968, Vol. 11, p. 454. [11] Meieran, E. S., Rev. Sci. Instrum., 33 (1962) , 319. [12] Lopata, S. L. and Kula, E. B., Trans. AIME, 224 (1962) , 865. [13] Leber, S., Rev. Sci. Instrum., 36 (1965) , 1747. [14] Elias, J. A. and Heckler, A. J., Trans. AIME, 239 (1967) , 1237. [15] Schuiz, L. G., J. Appl. Phys., 20 (1949) , 1030. [16] Morris, P. R., Texture Cryst. Sol., 2 (1976) , 57. [17] Jura, J. and Pospiech, J., Texture Cryst. Sol., 2 (1976) , 81. [18] Bunge, H. J., Tobisch, J. and Mucklich, A., Texture, 1 (1974) , 211. [19] Humbert, M., Wagner, F. and Baro, R., Texture Cryst. Sol., 3 (1978) , 27. [20] Davies, G. J., Goodwill, D. J. and Kallend, J. S., J. Appl. Cryst., 4 (1971) , 67. [21] Hu, H., in Recovery and Recrystallization of Metals, Interscience Publishers, New York, 1963, p. 311. [22] Bunge, H. J., Phys. Status Solidi, 26 (1968) , 167. [23] Bunge, H. J. and Roberts, W. T., J. Appl., Cryst., 2 (1969) , 116. [24] Schlafer, D. and Bunge, H. J., Texture, 1 (1974) , 157. [25] Bunge, H. J., Schleusener, D. and Schlafer, D., Met. Sci. J., 8 (1974) , 413. [26] Hechler, A. J. and Granzow, W. G., Met. Trans., 1 (1970) , 2089. [27] Inagaki, H. and Suda, T., Texture, 1 (1973) , 129. [28] Willis, D. J. and Hatherly, M., in Texture and Properties of Materials, 4th Int. Conf. on Texture, Cambridge, The Metals Society, 1976, p. 48. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|