| 硅钢热轧卷焊接接头断裂因素的研究 |
| 戚濂;浦绍康;殷碧群 |
| 武汉钢铁公司钢铁研究所;武汉钢铁公司钢铁研究所;武汉钢铁公司钢铁研究所 |
|
| SOME FACTORS AFFECTING THE WELDED JOINT FRACTURE IN HOT-ROLLED SILICON STEEL COIL |
| Qi Lian;Pu Shaokang;Yin Biqun Research Institute of Wuhan Iron and Steel Company |
引用本文:
戚濂;浦绍康;殷碧群. 硅钢热轧卷焊接接头断裂因素的研究[J]. 金属学报, 1980, 16(3): 331-377.
,
,
.
SOME FACTORS AFFECTING THE WELDED JOINT FRACTURE IN HOT-ROLLED SILICON STEEL COIL[J]. Acta Metall Sin, 1980, 16(3): 331-377.
[1] Hull, D., Acta Met., 9 (1961) , 191. [2] Gell, M. and Worthington, P. J., Acta Met., 14 (1966) , 1265. [3] Worthington, P. J. and Smith, E., Acta Met., 14 (1966) , 35. [4] Anderson, E. and Spreadborough, J., J. Iron Steel Inst., 206 (1968) , 1223. [5] Leslie, W. C., Fischer, R. M. and Sen, N., Acta Met., 7 (1959) , 632. [6] Leslie, W. C., Rickett, R. L., Stroble, C. P. and Konoval, G., Trans. ASM, 53 (1961) , 715. [7] Konoval, G., Zwell, L., Dorman, L. A. and Leslie, W. C., Nature, 184 (1959) , 1863. [8] McMahon, C. J. Jr. and Cohen, M., Acta Met., 13 (1965) , 591. [9] Aronsson, B. and Granas, L., Met. Trans., 2 (1971) , 1087. [10] McMahon, C. J. Jr., Acta Met., 14 (1966) , 839. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|