| 冰晶石-氧化铝熔液对炭电极的湿润 |
| 邱竹贤;魏庆斌 |
|
| ON THE WETTABILITY OF CARBON ELECTRODES BY MOLTEN CRYOLITE-ALUMINA ELECTROLYTE |
| Qiu Zhuxian and Wei Chingbin |
引用本文:
邱竹贤;魏庆斌. 冰晶石-氧化铝熔液对炭电极的湿润[J]. 金属学报, 1980, 16(3): 357-361.
,
.
ON THE WETTABILITY OF CARBON ELECTRODES BY MOLTEN CRYOLITE-ALUMINA ELECTROLYTE[J]. Acta Metall Sin, 1980, 16(3): 357-361.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|