| 氮化层的断裂力学分析 |
| 胡义祥 |
| 大连机车车辆工厂试验室 |
|
| FRACTURE MECHANICS ANALYSIS OF THE NITRIDED CASE ON NODULAR CAST IRON |
| Hu Yixiang Dalian Locomotive Works |
引用本文:
胡义祥. 氮化层的断裂力学分析[J]. 金属学报, 1980, 16(4): 463-469.
.
FRACTURE MECHANICS ANALYSIS OF THE NITRIDED CASE ON NODULAR CAST IRON[J]. Acta Metall Sin, 1980, 16(4): 463-469.
[1] 浅见克敏,寺沢正男,吉岡靖夫,日本机械学会论文集 42(1976) ,989. [2] Barson, J. M. and Mcnicol, R. C., Amer. Soc. Test. Mater., Spec. Tech. Publ., № 559, 1974, p. 183. [3] 范天佑,断裂力学基础,江苏科学技术出版社,1978,p.328. |
|