| 铁基高温合金中μ相和σ相引起的晶界脆化 |
| 陈国良;谢锡善;倪克铨;徐志超;王迪;张明;居玉英 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;上海钢铁研究所;上海第五钢铁厂 |
|
| GRAIN BOUNDARY EMBRITTLEMENT BY μ AND σ PHASES IN IRON-BASE SUPERALLOYS |
| Chen Guoliang; Xie Xishan; Ni Kequan; Xu Zhichao; Wang Di (Beijing Institute of Iron and Steel Technology); Zhang Ming (Shanghai Institute of Iron and Steel Research); and Ju Yuying (Shanghai No. 5 Steel Works) |
引用本文:
陈国良;谢锡善;倪克铨;徐志超;王迪;张明;居玉英. 铁基高温合金中μ相和σ相引起的晶界脆化[J]. 金属学报, 1981, 17(1): 1-114.
,
,
,
,
,
,
.
GRAIN BOUNDARY EMBRITTLEMENT BY μ AND σ PHASES IN IRON-BASE SUPERALLOYS[J]. Acta Metall Sin, 1981, 17(1): 1-114.
[1] Sullivan, C. P. and Donachie, M. J., Jr., Metals Eng. Quart.,11(1971) , № 4, 1. [2] Decker, R.F. and Floreen, S., Precipitation from Iron-Base Alloys, Eds. G. R. Speich and J. B. ClarK,Gordon and Breach, New York, 1965, p. 69. [3] Sims, C. T., J. Metals, 18 (1966) , 1119. [4] Sabol, G, P, and Stickler, R., Phys. Status Solidi, 35 (1969) , 11. [5] Sims, C. T., The Superalloys, Eds. C. T. Sims and W. C. Hagel, John Wiley & Sons, New York 1972, p. 259. [6] Sullivan, C. P. and Donachie, M. J., Jr., Metals Eng. Quart., 7 (1967) ,№ 1, 36. [7] Mihalisin, J. R., Bieber, C. G. and Grant, R. T., Trans. AIME, 242 (1968) , 2399. [8] 陈淦生、姚常春、仲增墉,金属学报,14(1978) ,284. [9] Beattie, H. J., Jr., and Hagel, W. C., Trans. AIME, 221 (1961) , 28. [10] Maniar, G. N., Muzyka, D. R. and Whitney, C. R., Trans. AIME, 245 (1969) , 701. [11] Wood, J. R., Proe. 3rd Int'l Symp. on Superalloys, Seven Springs, Pa. 1976, p. 227. [12] 北京钢铁学院高温合金研究组,金属学报,14(1978) ,440. [13] 上海钢铁研究所,北京钢铁学院,15Cr-40Ni型铁基高温合金的研究报告,1978. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|