| CoO孕育剂促进铸造镍基高温合金晶粒细化的研究 |
| 赵惠田;师昌绪 |
| 中国科学院金属研究所;中国科学院金属研究所 |
|
| INVESTIGATION OF CoO INOCULANT FOR SURFACE GRAIN REFINEMENT OF CAST NICKEL-BASE SUPERALLOY BLADES |
| Zhao Huitian and Shi Changxu (Institute of Metal Research; Academia Sinica) |
引用本文:
赵惠田;师昌绪. CoO孕育剂促进铸造镍基高温合金晶粒细化的研究[J]. 金属学报, 1981, 17(2): 118-123.
,
.
INVESTIGATION OF CoO INOCULANT FOR SURFACE GRAIN REFINEMENT OF CAST NICKEL-BASE SUPERALLOY BLADES[J]. Acta Metall Sin, 1981, 17(2): 118-123.