| 高温铝钎料的选择及其与母材的相互作用 |
| 张启运;刘淑祺 |
| 北京大学化学系;北京大学化学系 |
|
| SELECTION OF FILLER METAL FOR ALUMINUM BRAZING AND ITS REACTION WITH BASE METAL |
| by Zhang Qiyun and Liu Shuqi (Dept. of Chemistry; Beijing University) |
引用本文:
张启运;刘淑祺. 高温铝钎料的选择及其与母材的相互作用[J]. 金属学报, 1981, 17(3): 300-377.
,
.
SELECTION OF FILLER METAL FOR ALUMINUM BRAZING AND ITS REACTION WITH BASE METAL[J]. Acta Metall Sin, 1981, 17(3): 300-377.
[1] Schoer, H., Schultze, W., Ger. Pat. Nr. 1962 760. [2] Miller, M. A., Weld. J., 25 (1946) , 102-s. [3] 川勝一郎,大泥直,日本金属学会誌,35(1971) ,53. [4] 张启运,郑朝贵,刘淑祺,金属学报,15(1979) ,109. [5] 1977. [6] Hansen, M., Constitution of Binary Alloys, McGraw-Hill, New York, 1958. [7] 西成基,篠田武雄,和出升,轻金属,22(1972) ,716. [8] Jenkinson, D. C., Hogan, L. M., J. Cryst. Growth, 28 (1975) , 171. [9] 张启运,郑朝贵,韩万书,金属学报,17(1981) ,130." |
|