高法向塑性的各向异性冷轧和退火磷钢板材的弹性性质 |
胡郇 |
美国钢铁公司研究所 |
|
ELASTIC PROPERTIES OF COLD-ROLLED AND ANNEALED SHEETS OF PHOSPHORUS STEEL HAVING HIGH NORMAL PLASTIC ANISOTROPY |
Hsun Hu (U. S. Steel Research Laboratory; Monroeville; Pa 15146; U.S.A.) |
引用本文:
胡郇. 高法向塑性的各向异性冷轧和退火磷钢板材的弹性性质[J]. 金属学报, 1981, 17(6): 595-606.
.
ELASTIC PROPERTIES OF COLD-ROLLED AND ANNEALED SHEETS OF PHOSPHORUS STEEL HAVING HIGH NORMAL PLASTIC ANISOTROPY[J]. Acta Metall Sin, 1981, 17(6): 595-606.
[1] Hu, H., 待发表. [2] Roe, R. J., J. Appl. Phys,, 36 (1965) , 2024. [3] Roe, R. J., ibid., 37 (1966) , 2069. [4] Bunge, H. J., Z. Metallk., 56 (1965) , 872. [5] Bunge, H. J., Mathematische Methoden der Texturanalyse, Akademie-Verlag, Berlin, 1969. [6] Bunge, H. J., Ebert, R. and Gunther, F., Phys. Status Solidi, 31 (1969) , 565. [7] Kallend, J. S. and Davies, G. J., J. Inst. Met., 98 (1970) , 242. [8] Kallend, J. S. and Davies, G. J., ibid., 99 (1971) , 257. [9] Morris, P. R., Int. J. Eng. Sci., 8 (1970) , 49. [10] Morris, P. R., Metall. Trans., 2 (1971) , 1949. [11] Bunge, H. J. and Roberts, W. T., J. Appl. Cryst., 2 (1969) , 116. [12] Voigt, W., Lehrbuch der Kristallphysik, Teubner Verlag, Leipzig, 1928, p. 739. [13] Reuss, A., Z. Angew. Math. Mech., 9 (1929) , 49. [14] Hill, R., Phys. Soc. Proc. (London), 65 (1952) , 349. [15] Chung, D. H. and Buessem, W. R., J. Appl. Phys., 38 (1967) , 2535. [16] Kroner, E., Z. Phys., 151 (1958) , 504. [17] Bunge, H. J., Krist. Tech., 3 (1968) , 431. [18] Morris, P.R., J. Appl. Phys., 40 (1969) , 447. [19] Nye, J. F., Physical Properties of Crystals, Clarendon Press, Oxford, 1957, p. 135. [20] Mason, W. P., Piezoelectric Crystals and Their Application to Ultrasonics, Van Nostrand, 1950, p. 417. [21] Nye, J. F., Physical Properties of Crystals, Clarendon Press, Oxford, 1957, p. 147. [22] Stickels, C. A. and Mould, P. R., Metall. Trans., 1 (1970) , 1303. [23] Mould, P. R. and Johnson, T. E., Jr., Sheet Met. Ind., 50 (1973) , 328; 348. [24] Alers, G. A. and Liu, Y. C., Trans. Metall. Soc. AIME, 236 (1966) , 482. [25] Liu, Y. C. and Alers, G. A., ibid., 236 (1966) , 489. [26] Zener, C., Elasticity and Anelasticity of Metals, Univ. Chicage Press, 1956, p. 7. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|