| Cr含量对30CrNi5MoV钢“软化”效应的探讨 |
| 鲁肇俊;吴宝榕;吴佩芝;李桂芬;王琪;卢鸿修;李雪缘;金钦乾;汪德根 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| INFLUENCE OF Cr ON "SOFTENING EFFECT" OF 30CrNiSMoV STEEL |
| Lu Zaojun; Wu Baorong; Wu Peizhi; Li Guiyen; Wang Qi; Lu Hongxiu; Li Xueyuan; Jin Qingqian; Wang Degen (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
引用本文:
鲁肇俊;吴宝榕;吴佩芝;李桂芬;王琪;卢鸿修;李雪缘;金钦乾;汪德根. Cr含量对30CrNi5MoV钢“软化”效应的探讨[J]. 金属学报, 1982, 18(1): 85-134.
,
,
,
,
,
,
,
,
.
INFLUENCE OF Cr ON "SOFTENING EFFECT" OF 30CrNiSMoV STEEL[J]. Acta Metall Sin, 1982, 18(1): 85-134.
1 Lacy, C. E.; Gensamer, M., Trans. ASM, 32 (1944) , 88. 2 Leslie, W. C.; Sober, R. J.; Babcock, S. G.; Green, S. J., ASM Trans. Q., 62 (1969) , 691. 3 Leslie, W. C., Metall. Trans., 3 (1972) , 5. 4 Tanaka, T.; Watanabe, S., Acta Metall., 19 (1971) , 991. 5 Ulitchny, M. G.; Vasndevan, A. K.; Gibala, R., The Microstructure and Design of Alloys, Proc. 3rd Int. Conf. on the Strength of Metals and Alloys, Vol. 1, Cambridge, England, 1973, p. 505. 6 Spitzig, W. A.; Leslie, W. C., Acta Metall., 19 (1971) , 1143. 7 Spitzig, W. A., Mater. Sci. Eng., 16 (1974) , 169. 8 Kelley, M. J.; Stoloff, N. S., Metall. Trans., 7A (1976) , 331. 9 Thomas. G., Iron Steel Int., 46 (1973) . 451. 10 小林泽;白沢秀则;自在丸二郎,铁钢,66(1980) ,685. 11 Ansell,G.S.未发表资料;1979. 12 Bush, M. E.; Kelly, P. M., Acta Metall., 19 (1971) , 1363. 13 Bergstroem, Y.; Josefsson, ■., Scan. J. Metall., 3 (1974) , 259. 14 Norstroem, L.-■., Scan, J. Metall., 5 (1976) , 41. 15 Smith, D. W.; Hehemarm, R. F., J. Iron Steel Inst., 209 (1971) , 476. 16 Naylor, J. P., Metall. Trans., 10A (1979) , 861. 17 Irvine, K. J.; Pickering, F. B., J. Iron Steel Inst., 201 (1963) , 944.L |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|