| α-Fe,γ-Fe和Fe_4N的价电子和磁矩结构分析——α-Fe→γ-Fe相变、高温渗氮表面硬化、渗碳体石墨化及其它材料的电子理论 |
| 余瑞璜 |
| 吉林大学物理系及暨南大学固体与分子理论与应用研究室 |
|
| ANALYSIS OF VALENCE ELECTRON AND MAGNETIC MOMENT STRUCTURES OF α-Fe, γ-Fe AND Fe_4N——ELECTRON THEORY OF CASE HARDENING, α-TO γ-Fe PHASE TRANSFORMATION AND CERTAIN OTHER RELATED PROCESSES |
| Yu Ruihuang (S. H. Yu) (Department of Physics; Jilin University; Changchun; Solid and Molecular Research Group; Jinan University; Guangzhou ) |
引用本文:
余瑞璜. α-Fe,γ-Fe和Fe_4N的价电子和磁矩结构分析——α-Fe→γ-Fe相变、高温渗氮表面硬化、渗碳体石墨化及其它材料的电子理论[J]. 金属学报, 1982, 18(3): 336-349.
.
ANALYSIS OF VALENCE ELECTRON AND MAGNETIC MOMENT STRUCTURES OF α-Fe, γ-Fe AND Fe_4N——ELECTRON THEORY OF CASE HARDENING, α-TO γ-Fe PHASE TRANSFORMATION AND CERTAIN OTHER RELATED PROCESSES[J]. Acta Metall Sin, 1982, 18(3): 336-349.
1 余瑞璜(S.H.Yu),科学通报,23(1978) ,217. 2 Mattheiss, L. F., Bull. Am. Phys. Soc., Ser. Ⅱ, 8 (1963) , 222; Phys. Rev., 133 (1964) , A 1399. Seitz, F., The Modern Theory of Solids, McGraw-Hill, New York, 1940, p. 423, Fig. 4. 3 Landolt-Boernstein, I Baund, Atom-und Molekularphysik, 1 Teil, Atome und Ionen, Springer-Verlag, Berlin, 1950, p 60. 4 Mott, N. F.; Jones, H., The Theory of Properties of Metals and Alloys, Oxford Univ. Press, London, 1936, Chapt. 6. 5 Pauling, L., Proc. R. Soc., London, A196 (1949) , 343. 6 王奎雄,王兆民;陈雅符,科学通报、数理化专辑,(1980) ,176. 7 陈雅符;王奎雄;王兆民,科学通报,25(1980) ,974. 8 余瑞璜,科学通报,26(1981) ,206. 9 Hume-Rothery, W.; Raynor, G. V., The Structure of Metals and Alloys, 4th ed., Institute of Metals, London, 1962, p. 198. 10 余瑞璜,Science Reports(暨南大学学报特刊),(1980) ,№1,31. 11 Anderson, J. R.; Gold, A. V., Phys. Rev., 139 (1965) , A 1459. 12 Loucks, T. L., Phys, Rev. Lett., 14 (1965) , 1072. 13 Bizette, H.; Tsai, B., C. R. Hebd. Seances Acad. Sci., 236 (1940) , 252; Bizette, H., J. Phys. Radium, 12 (1951) , 161; Mashiyama, Y.; Uchida, E.; Kendoh, H., Busseiron Ken Kyu (Researches on Chemical Physies), 71 (1954) , 9; Roth, W. L., Phys. Rev., 110 (1958) , 1333; 111 (1958) , 772; Shull, C. G.; Strauser, W. A.; Wollan, E. O., Phys. Rev., 83 (1951) , 333. 14 Teble, R. S.; Graik, D. J., Magnetic Materials, John Wiley, London, 1969 p. 51, Table 2. 16. 15 Abrahams, S. C.; Guttman, L.; Kasper, J. S., Phys. Rev., 127 (1962) , 2052. 16 Bozorth, R. M., Ferromagnetism, D. Van Nostrand Co., Inc., New York, 1953, p. 809. 17 余瑞璜,渗碳体价电子结构分析(待发表) 18 余瑞璜,吉林大学自然科学学报,4(1978) ,54. 19 Thomas, E., J. Sci Instrum., 25 (1948) , 440. 20 Esser, H.; Eusterbrook, H., Arch. Eisenhuettenwes., 14 (1941) , 341; Nid, F. C.; Marnair, D., Phys. Rev., 64 (1941) , 597. 21 Shull, C. G.; Yamada, Y., J. Phys. Soc. Jpn., 17 Suppl. Bill (1962) , 1. Shull, C. G.; Mook, H. A., Phys. Rev. Lett., 16 (1966) , 184. 22 DeCicco, P. D.; Kitz, A., Phys. Rev., 162 (1967) , 486. 23 Frazer, B. C., Phys. Rev., 112 (1958) , 751. 24 Goodenough, J. B., Magnetism and the Chemical Bound, John Wiley & Sons, New York, 1963, p. 342. 25 Jack, K. H., Proc. R. Soc.London, A 195 (1949) , 34. 26 Herzberg, Z., Molecular Spectra of Molecular Structure 1, Spectra of Diatomic Molecules, D. Van Nostrand Co. Inc. Princeton, New York, 1951, p. 243-346, Table 34. , p. 553. 27 Bozorth, R. M., Ferromagnetism, D. Van Nostrand co., Inc., New York, 1953, p. 478. 28 Meyer, A. J. P.; Asch, G., J. Appl. Phys., 32 (1962) , 330.d |
|